Not quite. It means that on 12 spoons and 12 forks there should have been about 45 grams when they were new. The spoons should have a bit more silver on them than the forks because they have a slightly higher surface area. So it's closer to 1/24 of 45 grams per piece, so closer to 1.875 grams per piece, minus what has been lost to wear over the years.Oxygene said:Thanks to everyone, figured out finding the Internet.
Labeled "90" and "45" this means on one spoon about 1/12 of 45 grams, (about 3.75 grams) of pure silver were applied.