D dbrick81 Member Joined Dec 29, 2007 Messages 17 Location Delaware Jan 1, 2008 #1 Has anyone tried to make Stannous chloride from 95/5 (95 tin/5 antimony) plumbing solder. Do you think it would work or would the 5% antimony cause some problems? Thanks
Has anyone tried to make Stannous chloride from 95/5 (95 tin/5 antimony) plumbing solder. Do you think it would work or would the 5% antimony cause some problems? Thanks
Noxx Well-known member Joined Feb 24, 2007 Messages 3,365 Location Quebec, Canada Jan 1, 2008 #2 I used that many times and it works.