stannous chloride test solution

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

herbbartley

Member
Joined
Aug 18, 2011
Messages
12
Is the solution supposed to be diluted? I dissolved as much tin in 30ml of muriatic acid as it would take up and it is yellow in color, not clear.
 
was the tin pure? do not dilute. did you test on a solution that contained gold or other PM? if not, try it and see if it works.
 
Look on Lasersteves site he has a video of making stannous chloride and a testing solution for gold.
Mark
 

Latest posts

Back
Top