You can always rejuvenate it with more stannous.With my stannous,I just keep adding pieces of tin as they dissolve.The last batch I made I kept using for about 6 months,until I finally gave it to a someone last week.
If you just want to start with fresh,then you can raise the ph to 6+ with soda and discard