ok ok rite then let me ask sumthink , im not to up to date with the process of stripping and the stuff used ap i see people sayin, but say i did a batch ov gold in the ap wud i have to get the gold out or is there a ammount ov time i can leave the gold liquid sitting there ? cud i wait till i wanted to do a 2nd run and run the same liquid? ///,, chears for replys to all beforhand kev
 
uksmoker said:
ok ok rite then let me ask sumthink , im not to up to date with the process of stripping and the stuff used ap i see people sayin, but say i did a batch ov gold in the ap wud i have to get the gold out or is there a ammount ov time i can leave the gold liquid sitting there ? cud i wait till i wanted to do a 2nd run and run the same liquid? ///,, chears for replys to all beforhand kev
I realize I'm an old geezer, well behind the times, but I think you'd get a more serious reply to your inquiry if you'd lose the text messaging lingo. Please try to post your questions using common English. All of it!

I have a hard time taking anyone seriously that is too lazy to use an acceptable form of communication. If it's not worth it to you to pose a question properly, it certainly isn't worth my time to respond. Others, of course, may see the matter differently.

Harold
 
sorry people im not the sharpest tool in the box at the best of times, and ive just quit smokeing weed after 9 years straight so bare with me head still gettin used to the cleaness, i have watched videos show ap liquid disolving the gold , my question is when the gold is disovled do u have to do the next step straight away or can u leave the ap with gold in sitting for a in-def-e-nut time and use it for the next batch thus uppin the ammount ov gold in the liquid with out upping the batch size, kev
 
AP is for stripping not the best for dissolving. Filter the gold in a coffee filter then save it dry . Save the AP and add more Peroxide to reactivate the solution next time you go to RECOVER more gold plating. Notice recover in caps, use HCl+Cl to dissolve gold foils. I hope that helps.
 