- Joined
- Mar 19, 2021
- Messages
- 92
As Nick said. If you do not, look into the Iodine/Iodide leach. Components like this lend themselves to surface leaching rather than dissolving the 99.9% base metals to get at the roughly 1g per Kg they yield.If the product is all the same item which from your picture it seems to be then if you have access to cyanide that would be my process of choice.