Stephen Swartz
Active member
- Joined
- Feb 7, 2024
- Messages
- 40
What type of pH test strips would work good in agua regia and others please advise thank you
There are no specific test strips for Aqua Regia, but anything from 7-0 will do.What type of pH test strips would work good in agua regia and others please advise thank you
Drasil I haven't decided which process to use yet the blue liquid came from a nitric bath that I soaked my concentrates in and then dissolved a piece of copper in there also but why on the stanis chloride test would it be giving me an instant deep dark blackThere are no specific test strips for Aqua Regia, but anything from 7-0 will do.
But there are really not much need for pH tests if you dissolve Gold with AR.
It is mandatory if you dissolve foils or powders in HCl/ Bleach though.
DO NOT add acids to unknown rocks sand or Ore unless you have an assay.Drasil I haven't decided which process to use yet the blue liquid came from a nitric bath that I soaked my concentrates in and then dissolved a piece of copper in there also but why on the stanis chloride test would it be giving me an instant deep dark black
DO NOT add acids to unknown rocks sand or Ore unless you have an assay.
You have no idea what it might contain.
Since you added Copper (Why did you do that by the way?) no wonder it is blue.
Copper do react with Stannous some times and create a dark brownish/greyish black.
It is considered a false positive.
Nobody use Aqua Regia on ore!Drasil the ore that I have is sulphide base from porphory intrusion lots of pyrite chalcopyrite silver gold copper telluride's what I want to do is the agua regia process but due to the high silver content of this or I want to get both the gold and silver and according to the mine reports there should also be small amounts of platinum palladium and this specific mine back in the day produced over 450,000 oz of tellurium
And I would simply appreciate so very much plain simple in English instructions on how to do the agua regia process for this type of ore thanks
If there is Silver in the Solution one can not use Stannous, since it will drop Silver as Silver Chloride.I stuck two pieces of thin copper wire in there to see if any silver would precipitate
If there is Silver in the Solution one can not use Stannous, since it will drop Silver as Silver Chloride.
Yes delirium is mildly toxic to the radioactivity it does not exist in such extent that it is a danger to me I am also aware of the dangers of the gas is produced I am taken and am actively taking appropriate precautions....Drasil I'm not going to use agua regia on the oar I am going to use the agua regia on flash floated concentrate s that have already been put through a nitric acid soak please help me make this reality safely which I'm asking you because I'm going to do it either way is there a specific publication or video that details the aqua regia process and how after everything is dissolved to extract the silver first and then the gold please advise sir I would appreciate it very muchNobody use Aqua Regia on ore!
It is way to expensive and gives too much waste to treat.
Additionally Tellurium is mildly toxic by itself.
Have you read the links I gave you?
My phone number is 415-694-1926 if you're comfortable communicating with me there I would appreciate it very much this app is driving me up a wallNobody use Aqua Regia on ore!
It is way to expensive and gives too much waste to treat.
Additionally Tellurium is mildly toxic by itself.
Have you read the links I gave you?
You really need to study, for your own sake.Yes delirium is mildly toxic to the radioactivity it does not exist in such extent that it is a danger to me I am also aware of the dangers of the gas is produced I am taken and am actively taking appropriate precautions....Drasil I'm not going to use agua regia on the oar I am going to use the agua regia on flash floated concentrate s that have already been put through a nitric acid soak please help me make this reality safely which I'm asking you because I'm going to do it either way is there a specific publication or video that details the aqua regia process and how after everything is dissolved to extract the silver first and then the gold please advise sir I would appreciate it very much
I'm in different time zone.My phone number is 415-694-1926 if you're comfortable communicating with me there I would appreciate it very much this app is driving me up a wall
I have no idea of other membersI'm in different time zone.
So telephone is not an option.
There should be several good members in your general area/state.
Just show some patience, we do not lie inside the forum you know.I have no idea of other members
but it would be at your convenience sir if I need to stay up until 2:00 a.m. in the morning to speak with you that would be fine can you please give me a reference for the aqua regia process and how to extract my silver and gold from like I said I needed in simple terms
Well I never thought that sir and you however seem extremely knowledgeableJust show some patience, we do not lie inside the forum you know.