happy new 2020 for everyone here
i have crashing gold ore west already pahing by Ag prossess and removing gold from it 10 grams / /100 kg heap
. i smelt it iin tank with 600 gram thiourea powder .. now it has 12 hours and solution becam honey color .. i put active carbone iiside net cloth on the solutiion 300 gram and it give like bubbles .. i remove the soluution from tiime too time as i read little about CIL prossess ..
please tell me what the next to do
haw to remove gold from activ carbon by ashing and smelting ..
what the safety i should take to protect my self and invironment around me ..
i hope my engilsh enough to pass me idea for you ..
witng for more detils about thieorea prossess from a to z
i have crashing gold ore west already pahing by Ag prossess and removing gold from it 10 grams / /100 kg heap
. i smelt it iin tank with 600 gram thiourea powder .. now it has 12 hours and solution becam honey color .. i put active carbone iiside net cloth on the solutiion 300 gram and it give like bubbles .. i remove the soluution from tiime too time as i read little about CIL prossess ..
please tell me what the next to do
haw to remove gold from activ carbon by ashing and smelting ..
what the safety i should take to protect my self and invironment around me ..
i hope my engilsh enough to pass me idea for you ..
witng for more detils about thieorea prossess from a to z