A
Anonymous
Guest
Hello members,
I'm wanting to know what should I use to clean my beakers so I can reuse them.
The beakers I'm referring to at the moment were used to refine silver from keyboard mylars.
What has been used....
* Nitric Acid (69.5%)
* Peroxide (3%)
* Distilled Water.
I'm trying to reuse the beakers to start working with my sulfuric cell.
Thanks
Kevin
I'm wanting to know what should I use to clean my beakers so I can reuse them.
The beakers I'm referring to at the moment were used to refine silver from keyboard mylars.
What has been used....
* Nitric Acid (69.5%)
* Peroxide (3%)
* Distilled Water.
I'm trying to reuse the beakers to start working with my sulfuric cell.
Thanks
Kevin