We had 2 grams of gold. It sat I water for a week and turned black. I put the gold into a melting dish with borax and melted into a bead about 12mm in size. Put the bead into a cuppel with 3 grams lead into the furnace at 1700. Came back in 40 minutes. And there was nothing in the cuppel. Not gold no red lead oxide. The dish if the cuppel was black with no metallics. Split the cuppel and there is a dark gray sparkling layer about 2mm thick, but no gold present. Where did the gold go? Need some help.
 
We had 2 grams of gold. It sat I water for a week and turned black. I put the gold into a melting dish with borax and melted into a bead about 12mm in size. Put the bead into a cuppel with 3 grams lead into the furnace at 1700. Came back in 40 minutes. And there was nothing in the cuppel. Not gold no red lead oxide. The dish if the cuppel was black with no metallics. Split the cuppel and there is a dark gray sparkling layer about 2mm thick, but no gold present. Where did the gold go? Need some help.
There is not enough information.

Anyway the "Gold" turning black should have been a wake up call.
Gold do not react to any single acid and definitely not Water.
How do you know it was Gold in there in the first place?

How was this Gold achieved.
As detailed as possible please.
Start material, how it was treated and the whole story.
 