I have some white metal connector pins almost matching silver in appearance but they did not dissolve in nitric, nor did they dissolve in
sulfuric with kno3. I tried to process because I thaught they were silver they were in a batch and most all dissolved but these. I thaught I may have needed more acid(s) which I added to no effect.
Any idea what type of metal they could be? I would post pic but my camera is not good enough to show the slight difference in appearence from silver.
If this helps they are from electrical sealed relays 30 amp resistive 800,000 life cycle.
thanks jim
sulfuric with kno3. I tried to process because I thaught they were silver they were in a batch and most all dissolved but these. I thaught I may have needed more acid(s) which I added to no effect.
Any idea what type of metal they could be? I would post pic but my camera is not good enough to show the slight difference in appearence from silver.
If this helps they are from electrical sealed relays 30 amp resistive 800,000 life cycle.
thanks jim