Moses Well-known member Joined Mar 15, 2024 Messages 67 Location Creswell Oregon Apr 11, 2024 #1 what is the best thing to do with this, trying to correct some mistakes I've already made don't know exactly what's all in here lol Attachments 17128623298758391332113359824719.jpg 1.4 MB · Views: 0
what is the best thing to do with this, trying to correct some mistakes I've already made don't know exactly what's all in here lol
A anarxi Well-known member Joined Oct 30, 2019 Messages 173 Apr 11, 2024 #2 maybe pour into a red bucket ?
Yggdrasil Moderator Staff member Moderator Joined Oct 30, 2015 Messages 8,146 Location Norway Apr 11, 2024 #3 Moses said: what is the best thing to do with this, trying to correct some mistakes I've already made don't know exactly what's all in here lol Click to expand... We have absolutely no Idea what you are showing us. So unless you care to explain, I can suggest a green bucket in stead of a red?
Moses said: what is the best thing to do with this, trying to correct some mistakes I've already made don't know exactly what's all in here lol Click to expand... We have absolutely no Idea what you are showing us. So unless you care to explain, I can suggest a green bucket in stead of a red?