Electrolytic Recovery Part 3. b.: Filtering Questions

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

lazersteve

Well-known member
Joined
Feb 27, 2007
Messages
7,334
Location
Florida
Please post your questions and comments on this tutorial here.

UPDATE:
I've added this photo of the filtered gold powder, it's still wet one day after filtering:

goldball.jpg


I'll have more updates as time permits.

UPDATE #2:
I've added this photo of the filtered gold powder, it's now dry two days after filtering and weighs 22.5 gms:

FullCell.jpg


Steve
 
hey steve i didnt let it sit over night after i diluted i filterd it with a vacume filter, look how the sulfuric comes out clean and ready to use agian,while all the gold stays in the filter.
 
PM,

The clean acid means no base metals are in it. How much scrap did you run thru the cell before filtering? The more scrap you process the more blue-green the acid becomes due to dissolved base metals.

I've got a vaccuum setup but don't use it much. I may break it out and save some time on my next batch.

Steve
 
those pins took time so i got about 3 pounds changed filters abot 2 times got a big chuck of mud ,i will run the mud thru hot water one or twice
did it all in one day ,will try to melt tommorro
 