I guess you'd call it a Copper(II)Chloride generator?

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

Acidrain

Well-known member
Supporting Member
Joined
Apr 17, 2024
Messages
61
Location
Oregon
I'm getting things ready to strip the foils off of goldfingers and made this.
It's two 2 gallon buckets, one perforated for the inner and the outer has a vet hole for generated gasses.
Inside there's 1/4 air tubing with #60 holes drilled in it for aeration with small bubbles.
 

Attachments

  • IMG_0338.jpg
    IMG_0338.jpg
    251.7 KB · Views: 1
  • IMG_0332.jpg
    IMG_0332.jpg
    412.2 KB · Views: 1
  • IMG_0333.jpg
    IMG_0333.jpg
    460.2 KB · Views: 2
  • IMG_0335.jpg
    IMG_0335.jpg
    304.5 KB · Views: 1
  • IMG_0337.jpg
    IMG_0337.jpg
    393.5 KB · Views: 0
Well damn! I didn't think of checking to see if the plastic fittings I used on the poly hose were acid proof. I opened the lid when I got home feom work this evening and found that the AP solution ate the tee fitting I used on the nice circular aerator I made 😳.
I deleted that and just dunked the hose down to the bottom.
Lesson - Check ALL parts used for compatibility with a system.
 