Amol Gupta
knowledgeSeaker2207
- Joined
- Dec 17, 2023
- Messages
- 42
I have dissolved some pure silver using nitric acid, I started of with a solution(approx 5ml) of nitric acid and distilled water with a pH of 1, after dissolving some silver approx(1.25-1.5g) with some silver still at the bottom the pH has dropped to close to 5.
I was wondering what should be the pH of the solution before I start cementing the silver using copper.
I was wondering what should be the pH of the solution before I start cementing the silver using copper.