goldsilverpro In Remembrance Moderator Emeritus Joined Mar 30, 2007 Messages 7,961 Location Benton, Arkansas Jul 8, 2018 #1 Hadn't seen this before. Attachments Rand Gold Refining.pdf 2.8 MB · Views: 211
g_axelsson Administrator Staff member Administrator Moderator Joined Nov 17, 2007 Messages 5,528 Location Sweden Jul 8, 2018 #2 Nice article, they really go into details for the processes. I even saw the word "tenor" used for silver content in the electrolyte in a silver cell. It's not only Dean that is using it. Göran
Nice article, they really go into details for the processes. I even saw the word "tenor" used for silver content in the electrolyte in a silver cell. It's not only Dean that is using it. Göran
anachronism Well-known member Supporting Member Joined May 31, 2016 Messages 3,320 Jul 9, 2018 #3 Of course it's not only Dean that uses it. 8) 8)
cuchugold Well-known member Joined Oct 25, 2017 Messages 243 Jul 21, 2018 #4 goldsilverpro said: Hadn't seen this before. Click to expand... Thanks for the document GSP. :G p.s.: Read the article twice. Learned a lot. Truly superb. Thanks again.
goldsilverpro said: Hadn't seen this before. Click to expand... Thanks for the document GSP. :G p.s.: Read the article twice. Learned a lot. Truly superb. Thanks again.
J Jordan1 Member Joined Feb 15, 2018 Messages 15 Sep 9, 2018 #5 Great read GSP, What book is that out of? Thanks
goldsilverpro In Remembrance Moderator Emeritus Joined Mar 30, 2007 Messages 7,961 Location Benton, Arkansas Sep 9, 2018 #6 Jordan1 said: Great read GSP, What book is that out of? Click to expand... I have no idea. The link just gave that one chapter, as you see it. Here's where I got it. Seems like it was a conference publication, put out by Saimm. http://www.saimm.co.za/Conferences/ExtractiveMetallurgyOfGold/0615-Chapter10.pdf
Jordan1 said: Great read GSP, What book is that out of? Click to expand... I have no idea. The link just gave that one chapter, as you see it. Here's where I got it. Seems like it was a conference publication, put out by Saimm. http://www.saimm.co.za/Conferences/ExtractiveMetallurgyOfGold/0615-Chapter10.pdf
J jimdoc Well-known member Joined Mar 12, 2007 Messages 4,945 Location Philadelphia Sep 9, 2018 #7 It looks like it may be called "THE EXTRACTIVE METALLURGY OF GOLD" from the top of alot of the pages.
It looks like it may be called "THE EXTRACTIVE METALLURGY OF GOLD" from the top of alot of the pages.
J jimdoc Well-known member Joined Mar 12, 2007 Messages 4,945 Location Philadelphia Sep 9, 2018 #8 4Metals posted this: "The Extractive Metallurgy of Gold in south Africa by Stanley details specifics to the process used at the Rand refinery." http://goldrefiningforum.com/phpBB3/viewtopic.php?f=60&t=5842&p=50495&hilit=THE+EXTRACTIVE+METALLURGY+OF+GOLD#p50495 https://books.google.com/books/about/The_Extractive_Metallurgy_of_Gold_in_Sou.html?id=elvsAAAAMAAJ
4Metals posted this: "The Extractive Metallurgy of Gold in south Africa by Stanley details specifics to the process used at the Rand refinery." http://goldrefiningforum.com/phpBB3/viewtopic.php?f=60&t=5842&p=50495&hilit=THE+EXTRACTIVE+METALLURGY+OF+GOLD#p50495 https://books.google.com/books/about/The_Extractive_Metallurgy_of_Gold_in_Sou.html?id=elvsAAAAMAAJ