What and where are they from?Do any of these contain silver/PD?View attachment 61575View attachment 61576
First you can sort them by resistors, capacitors inductors and so on.Do any of these contain silver/PD?View attachment 61575View attachment 61576
Nothing was sorted here.I know they always sorted and such, but couldn't one process them in bulk? I mean if i'm depopulating 100 boards i find taking the ICs like enough of a job, would it be such hindrance to recovery? It can't be worst than processing a simple cucl solution if you want to recover copper and maybe separate base metals.
Can see this dude successfully getting rid of most plastic, doing something similar where you can leave almost metal alone, then process it altogheter. I mean i do get it but i still find sorting as a huge waste of time, unless you bored and want to (which tends to be my case).
Gas is getting burned right away, I seen years ago one system where the gas is actually saved, also most dangerous part of the system, the bottles fill way faster than one would believe. When talking plastic alone, half that gas should be enough to power the whole reaction of plastic to fuel.
You need to take pictures so that the markings are visible.Do any of these contain silver/PD?View attachment 61575View attachment 61576