Brown sludge in my silver solution, what is it??

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
Ok problem solved.
I have dissolved eveything in the solution that I still have. 600ml of this solution took 43 grams of silver before it was exhausted. I have must added some "3rd nitric leech" there - that is why there was soo much unused acid.
After solution has cooled down I have put the same copper pieces and silver participated without any problems this time :)

Thanks for help :)
 