Shark said:
Thanks Snoman, I will give them all a test.
Thanks Jon, the budget right now is in the air, but things are changing, and more so with my next button. But the $100 is not out of range. The question is I do I buy more material or equipment? Decisions, decisions, :lol:

Shark,
For about double that Sreetips built a great vacuum filtration system. He has a good video. It was clear and simple enough that I was able to duplicate it myself for about =<$200 even here in Alaska. Works AWESOME!

https://youtu.be/letBcol2IB8

Above link to his video. Below, link to mine. (His is better!!!)

https://youtu.be/Fpdnp5npAQE

When your budget allows it’s worth it.

Scott




Sent from my iPhone using Tapatalk
 
ARMCO said:
Shark said:
Thanks Snoman, I will give them all a test.
Thanks Jon, the budget right now is in the air, but things are changing, and more so with my next button. But the $100 is not out of range. The question is I do I buy more material or equipment? Decisions, decisions, :lol:

Shark,
For about double that Sreetips built a great vacuum filtration system. He has a good video. It was clear and simple enough that I was able to duplicate it myself for about =<$200 even here in Alaska. Works AWESOME!

https://youtu.be/letBcol2IB8

Above link to his video. Below, link to mine. (His is better!!!)

https://youtu.be/Fpdnp5npAQE

When your budget allows it’s worth it.

Scott




Sent from my iPhone using Tapatalk

I have watched Sreetips video with a lot of interest. I have to admit there were a couple of items that I just didn't catch in his video that I did pick out of yours. I now think I might be able to work with something similar. I will be looking into the needed parts very soon.

Palladium said:
Wait til you chew thru your first large lot of high stainless!
It gets real exciting! Some go easy as pie. Others....... Not so much so.

I just bumped into what I think is tin, it sure looks like snot anyway, and started forming crystals as soon as it started to cool. The good side is that I ran these items separately as a test since they were unmarked. (but did test positive for gold)
 
Shark said:
ARMCO said:
Shark said:
Thanks Snoman, I will give them all a test.
Thanks Jon, the budget right now is in the air, but things are changing, and more so with my next button. But the $100 is not out of range. The question is I do I buy more material or equipment? Decisions, decisions, [emoji1]

Shark,
For about double that Sreetips built a great vacuum filtration system. He has a good video. It was clear and simple enough that I was able to duplicate it myself for about =<$200 even here in Alaska. Works AWESOME!

https://youtu.be/letBcol2IB8

Above link to his video. Below, link to mine. (His is better!!!)

https://youtu.be/Fpdnp5npAQE

When your budget allows it’s worth it.

Scott


Shark said:
I have watched Sreetips video with a lot of interest. I have to admit there were a couple of items that I just didn't catch in his video that I did pick out of yours. I now think I might be able to work with something similar. I will be looking into the needed parts very soon.


Well cool. Glad it helped.
 