Hi
Firstly, just like to say that this is an awesome forum full of knowledge. I have been reading posts for some time and apologise that I have taken until now to write a post.
I would really appreciate some advise here.
I am trying to create fine powdered silver for a project. I live in the UK and cannot purchase Nitric Acid. I have read concerning making "cold nitric" but unsure if I want to go down that route.
I am looking at buying 1kg of silver grain at a time and converting it into a fine powder. The grain is approximately 6mm each part.
What I am considering doing is purchasing a ball mill and milling it to a fine powder.
Does anyone have any experience in milling silver grain to powder or have any advice concerning powdering (that doesn't include nitric acid)?
Thank you very much in advance
Firstly, just like to say that this is an awesome forum full of knowledge. I have been reading posts for some time and apologise that I have taken until now to write a post.
I would really appreciate some advise here.
I am trying to create fine powdered silver for a project. I live in the UK and cannot purchase Nitric Acid. I have read concerning making "cold nitric" but unsure if I want to go down that route.
I am looking at buying 1kg of silver grain at a time and converting it into a fine powder. The grain is approximately 6mm each part.
What I am considering doing is purchasing a ball mill and milling it to a fine powder.
Does anyone have any experience in milling silver grain to powder or have any advice concerning powdering (that doesn't include nitric acid)?
Thank you very much in advance