I may have stumbled onto to something, before I left on my Saskatchewan trip I had a bucket of crushed cpu's waiting for to be smelted.
The bucket was loaded with flux Borax/Soda Ash/Sodium Nitrate left by the furnace on my return some water. On stirring it looks like the cpu ceramics the small bits that do not crush are completely dissolved into a mud.
I'm going to add some complete cpu's and see what happens, an will post the results when I know them.
Best Regards
G
The bucket was loaded with flux Borax/Soda Ash/Sodium Nitrate left by the furnace on my return some water. On stirring it looks like the cpu ceramics the small bits that do not crush are completely dissolved into a mud.
I'm going to add some complete cpu's and see what happens, an will post the results when I know them.
Best Regards