Hi
I was given 10.430 kg of telecomm boards made by DSC communication company.
So far I have depopulated and processed gold fingers and what I think is called a swtich from these boards.
Here is the recovered gold for each parts.
These are the boards
These are the gold fingers removed manually
So that makes the yield for these types of gold fingers to be 3.37 grams per kg (1.52 grams per lb)