@Spaceships a lot. Talking hundreds possibly a thousand or two. Not tonnes tho.
Thatsfunny said:My original question Is anyone familiar with this type? The insulator material seems to have a reaction to acid. I collected several hundred this last weekend.
FormidableRogue said:Side note. Hard drives are platinum plated....
goldsilverpro said:For Pt in hard drive disks, check my posts on the 1st page of this thread.
http://www.goldrefiningforum.com/phpBB3/viewtopic.php?f=63&t=14608&p=146892&hilit=hard+drive+disk+cobalt#p146892
To make a long story short, my conclusion is that, at today's Pt price, the disks that do contain Pt only contain about $.007 - $.035 of Pt per disk.