Today i've played with some fibre CPUs and a blowtorch.
The tiny gold-plated pins pop off all over the place, most of the weight is in the metal lid (if present) and the fibre catches fire. Fibre CPUs are a PITA.
Several hours after doing the 'playing', there is still a definite phenol smell in the air.
I'm Outside, and there's a light breeze, yet there is still occasionally that distinctive phenol smell about 4 hours later.
It could be that the phenol content is worth more than the gold content of fibre processors.