Geology, Geochemistry, Mineralogy, Metallurgy, Mineral Exploration, Mining Engineering, Ad Infinitum !!

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
Hi, is anyone able to use the links, because I've tried from a couple of PC's and they seem to be broken or the site no longer exists. If anyone has the site address that works, please post?
 
When the new software was implemented, many links were disabled. Report to moderators. If it can be fixed, they will take care of it when they get time.

Time for more coffee.
 
It's not a broken link like the links on the forum. I'm not sure what the issue is, but you can still access the books with a Google search. Go to Z-Library. The world's largest ebook library., then click on Books. There is a search there. Copy the title of the book you're interested in from the list in the first post and paste it into their search. I tried one and it seemed to work.

I'm slowly working through broken links here on the forum. I'm afraid it will be a while before I can circle back to this post and try to fix them all.

Dave
 
I fell down a deep hole on the internet trying to find Extractive Metallurgy 1: Basic Thermodynamics and Kinetics for some evening reading. I stumbled upon the attached PDF, "OPEN ACCESS E-BOOKS ON METALLURGICAL & MATERIALS ENGINEERING" Not sure who compiled this, but the links seem good and there are a lot of really old books in there. I pulled out a few that I've put on my reading list. This PDF contains links to 714 different books, papers, etc. regarding metallurgical processes. There isn't much regarding precious metals (just one or two papers) but hopefully there is something in there someone might enjoy reading.

INDUSTRIAL METALLURGY
175. The Fire Assay of Gold, Silver and Lead in Ores and Metallurgical Products by Leonard S. Austin (1907)

MATERIALS ENGINEERING
140. Gold Metallurgy and the Environment
142. The Chemistry of Gold Extraction

144. Partial Roasting of a PGM Concentrate Department of Materials Science and Metallurgical Engineering
55. Metallurgical Characterization of New Palladium-Containing CoCr and NiCr Alloys

Elemental
 

Attachments

  • Metallurgical.pdf
    996.2 KB · Views: 13
I fell down a deep hole on the internet trying to find Extractive Metallurgy 1: Basic Thermodynamics and Kinetics for some evening reading. I stumbled upon the attached PDF, "OPEN ACCESS E-BOOKS ON METALLURGICAL & MATERIALS ENGINEERING" Not sure who compiled this, but the links seem good and there are a lot of really old books in there. I pulled out a few that I've put on my reading list. This PDF contains links to 714 different books, papers, etc. regarding metallurgical processes. There isn't much regarding precious metals (just one or two papers) but hopefully there is something in there someone might enjoy reading.

INDUSTRIAL METALLURGY
175. The Fire Assay of Gold, Silver and Lead in Ores and Metallurgical Products by Leonard S. Austin (1907)

MATERIALS ENGINEERING
140. Gold Metallurgy and the Environment
142. The Chemistry of Gold Extraction

144. Partial Roasting of a PGM Concentrate Department of Materials Science and Metallurgical Engineering
55. Metallurgical Characterization of New Palladium-Containing CoCr and NiCr Alloys

Elemental
Thanks Elemental 😃
 
It's not a broken link like the links on the forum. I'm not sure what the issue is, but you can still access the books with a Google search. Go to Z-Library. The world's largest ebook library., then click on Books. There is a search there.
I know this is a bit old link/conversation. But when I try to open the link. I get a security warning stating that the link is reconnized as unsafe by my browser.
Is it still a good link, or has it been compromised?
Thanks much for your time and assistance.
 
Yeah, I'm getting a warning that the connection isn't private.

Someone else reported a similar error trying to get to Boardsort's site. Must be something new on the net.

Dave
 
It's not a broken link like the links on the forum. I'm not sure what the issue is, but you can still access the books with a Google search. Go to Z-Library. The world's largest ebook library., then click on Books. There is a search there. Copy the title of the book you're interested in from the list in the first post and paste it into their search. I tried one and it seemed to work.
I went to z-library today and got this message.
Looks like they are in the naughty corner!
 

Attachments

  • Screenshot 2022-12-14 23.33.15.png
    Screenshot 2022-12-14 23.33.15.png
    780.1 KB · Views: 0
Sorry you missed out Mech, I literally raped that site lol...

I got books you just can't find online from there (explosives safety, chemistry, etc...) I can spend time within that archive, which is on my computer, and list what books I possess. Then I will provide that listing for the membership if someone wishes to acquire any of these manuscripts.

I'll just warn everyone that this listing may be very large, and I'm pretty certain that it's going to be a candy shop for all the kids here (lol 😂🤣)...

If a means of transferring large files (some of these books are hundreds of megabytes in size) I'd be happy to upload them for the group.

I kid you not... I've got a respectable library of digital books (I estimate around 300 gigabytes) related to many of the topics discussed here...

That listing will most likely take me awhile to compose... So stand by
 
04/08/2016 07:27 PM 1,588,545 Nelson and Giles, 1985 (Hydrothermal Eruptions and Hot Spring Gold).pdf
04/16/2020 12:32 AM 946,449 New Gold Ore Occurrences in Carbonaceous Deposits.pdf
04/07/2020 10:20 PM 5,171,597 OROGENIC GOLD DEPOSIT IN MEXICO.pdf
04/07/2020 10:20 PM 121,970 Orogenic gold systems in the Andes of South America.pdf
07/30/2018 05:19 AM 440,684 Oxidation and Secondary Enrichment of Gold Deposits.pdf
03/22/2016 08:48 PM 6,000,985 placer-gold-recovery-methods.pdf
09/25/2011 09:58 PM 6,000,985 placer-gold.pdf
09/25/2011 10:22 PM 846,513 placer.pdf
06/15/2018 05:29 AM 7,541,913 Porphyry-Type Gold Mineralization.pdf
08/27/2020 01:36 PM 11,5u65,455 Potassic Igneous Rocks and Associated Gold-Copper Mineralization by Daniel Müller, David I. Groves (auth.) (z-lib.org).pdf
01/30/2019 02:55 PM 387,235 Proterozoic Lode Gold.pdf
01/30/2019 02:54 PM 918,414 RED LAKE GOLD MINES REPORT.pdf
08/16/2023 07:02 AM 693,492 Relativity and the nobility of gold.pdf
01/30/2019 02:54 PM 499,898 REPORT-MACANDREW RED LAKE GOLD MINES.pdf
07/26/2020 09:08 AM 4,830,152 Rhenium Content of Molybdenite in the Aitik Cu-Au-Ag-(Mo)Deposit.pdf
03/16/2016 11:30 PM 761,130 SEDIMENT-HOSTED AU DEPOSITS.pdf
07/25/2020 02:17 AM 386,379 Sedimentary Rock-Hosted Disseminated Precious Metal Mineralization - Peru.pdf
12/28/2010 08:15 AM 956,194 skarn gold deposits.pdf
03/23/2016 12:56 AM 729,013 Solubility of gold in arsenian pyrite.pdf
07/26/2020 08:24 AM 20,518,327 Specularite-Gold Mineralization.pdf
04/07/2020 10:20 PM 3,444,258 Structural Controls on gold mineralization on the margin of the Yilgarn craton, Australia - 2014.pdf
04/16/2020 12:32 AM 1,188,699 sulfate-hematite-sulfide zoningin the auriferous Mariana anticline.pdf
01/30/2019 02:55 PM 1,514,576 TECHNICAL REPORT-GOLD CENTRE MINE RED LAKE.pdf
05/27/2020 09:02 AM 814,344 Tectonics_and_distribution_of_gold deposits in China.pdf
09/20/2019 10:36 AM 650,424 The geomicrobiology of gold.pdf
06/15/2018 11:10 AM 14,629,041 THE GIANT-CON ARCHEAN LODE-GOLD SYSTEM DEPOSIT.pdf
08/20/2012 07:04 PM 4,371,387 The gold-seekers handbook and practical assayist.pdf
07/25/2020 02:17 AM 7,358,351 THE LEACHING AND ADSORPTION BEHAVIOUR OF GOLD ORES.pdf
01/10/2021 06:19 AM 71,859,299 The Metallogeny of Lode Gold Deposits. A Syngenetic Perspective by Kretschmar, Ulrich McBride, Derek (z-lib.org).pdf
08/20/2012 05:31 PM 19,180,753 The Metallurgy Of Gold By M Eissler.pdf
07/25/2020 02:17 AM 910,961 THE MINERALOGY OF THE BELLEROPHON-NELSON TELLURIDE-BEARING GOLD DEPOSIT.pdf
04/07/2020 10:20 PM 6,747,836 The Nature of Gold in the Aitik Cu-Au Deposit.pdf
01/30/2019 02:55 PM 4,441,384 The origin of the Archean Jardine iron formation-hosted lode gold.pdf
08/02/2020 09:13 AM 23,736,758 The_extractive_metallurgy_of_gold_in_South_Africa.pdf
08/26/2020 07:23 AM 8,751,513 Typomorphic features of the quartz of various mineral paragenesis from the gold mineralization in Karakshatau Mountains (West Uzbekistan).pdf
07/25/2020 02:17 AM 881,503 Understanding gold-(silver)-telluride-(selenide) mineral deposits.pdf
03/23/2016 04:18 AM 2,829,520 unusual gold mineralization.pdf
07/30/2018 04:57 AM 16,525,520 using applied geology to discover large copper and gold mines.pdf
07/30/2018 02:13 AM 53,205,486 Where-Find-is-Gold-in-World.pdf
04/07/2020 10:20 PM 6,511,235 zolowo gold_technical_presentation_-_q2_2019.pdf
01/08/2011 08:13 PM 5,311,616 [PDF] A SURVEY OF CONVENTIONAL AND NOVEL PROCESSES FOR THE TREATMENT OF GOLD.pdf
01/08/2011 07:54 PM 52,833 [PDF] ALTERNATES TO GOLD RECOVERY BY CYANIDE LEACHING.pdf
12/25/2010 01:21 AM 673,958 1975 - A process for the treatment of mixtures of platinum group metals and gold .pdf
12/25/2010 01:20 AM 638,306 1991 - The recovery of platinum-group metals and gold from sources containing same .pdf
12/25/2010 01:23 AM 2,430,965 2009Jones-ConRoast-CIM.pdf
04/16/2020 12:32 AM 2,119,219 2017_Platiniferous gold-tourmaline aggregates in the gold-palladium belt of Minas Gerais, Brazil.pdf
12/24/2010 07:20 AM 4,100,996 7-McClenaghan- Gold and PGE indicator mineral methods in mineral exploration IAGS 09.pdf
10/17/2019 11:46 PM 4,076,913 Andersen2017_Article_Platinum-groupMineralizationAt.pdf
03/30/2020 08:17 AM 1,086,209 Appendix_to_Platinum-Group_Element_Chromium and Vanadium Deposits in Mafic and Ultramafic Rocks.pdf
03/30/2020 08:17 AM 809,644 A_Unexpectedly_high-PGE_chromitite from the deeper mantle section.pdf
02/14/2020 07:42 PM 2,850,471 Chalcophile_and_platinum-group_element_concentrations in the sulfide minerals and the origin of PGE in pyrite Canada.pdf
12/13/2019 04:50 PM 667,136 Chapter 10_PGM_Guide.pdf
12/13/2019 04:50 PM 604,221 Chapter 1_PGM_Guide.pdf
12/13/2019 04:50 PM 631,872 Chapter 2_PGM_Guide.pdf
12/13/2019 04:50 PM 1,740,396 Chapter 3_PGM_Guide.pdf
12/13/2019 04:50 PM 104,395 Chapter 4_PGM_Guide.pdf
12/13/2019 04:50 PM 650,784 Chapter 5_PGM_Guide.pdf
12/13/2019 04:50 PM 865,925 Chapter 6_PGM_Guide.pdf
12/13/2019 04:50 PM 624,198 Chapter 7_PGM_Guide.pdf
12/13/2019 04:50 PM 907,688 Chapter 8_PGM_Guide.pdf
12/13/2019 04:50 PM 3,990,105 Chapter 9_PGM_Guide.pdf
02/19/2020 01:36 PM 10,831,800 Cu-Ni-PGE fertility of the Yoko-Dovyren layered massif.pdf
03/17/2016 02:52 AM 466,048 Determination of platinum metals in carbonaceous minerals.pdf
01/01/2011 07:13 PM 292,208 Determination of Platinum, Palladium, Rhodium and Titanium .pdf
01/21/2020 02:57 PM 2,425,250 DirectleachapproachestoPlatinumGroupMetalPGMoresandconcentrates.Areview.pdf
03/16/2016 10:46 PM 1,417,864 DISPERSION OF Pt Pd AND AU.pdf
08/19/2020 05:20 AM 1,220,684 East_Scandinavian_Mafic Large Igneous Provinces of Pd-Pt Ores.pdf
11/26/2019 07:23 PM 13,939,140 Economic Geology of the Platinum Metals.pdf
02/01/2020 11:55 PM 2,267,540 Enrichment_of_PGE_through_interaction_of _evolved boninitic magmas.pdf
06/21/2020 08:46 PM 38,340,960 Exploration_for_Platinum-Group_Elements (vol. 35).pdf
02/01/2020 11:55 PM 2,461,097 First_report_of_platinum-group_minerals.pdf
02/01/2020 11:55 PM 2,356,785 Footwall-type_Cu-Ni-PGE_Mineralization_in the Broken Hammer Area Sudbury Canada.pdf
01/07/2011 06:51 PM 449,285 Gilchrist-PGM procedures.pdf
03/03/2016 04:04 AM 1,686,389 GOLD-PLATINUM-PALLADIUM LODE IN NEVADA.pdf
03/16/2016 10:14 PM 218,893 gold_platinum_report.pdf
01/02/2020 09:06 PM 2,252,407 Hydrometallurgical recovery of platinum group metals.pdf
03/23/2016 02:42 AM 1,493,584 HYDROMETALLURGY-PGM.pdf
10/03/2019 05:20 AM 1,553,079 In_situ_Re_Os_isotopic_analysis_of_plati.pdf
12/13/2019 04:50 PM 687,738 IPA-Harmonised-Sampling-Procedure-of-Platinum-at-Workplace.pdf
10/17/2019 11:46 PM 468,108 Irarsite-hollingworthite and other pgms.pdf
01/04/2020 11:05 AM 3,836,531 Journal_of_the_VIRTUAL_EXPLORER.pdf
02/19/2019 07:31 AM 8,716,526 Magmatic Ore Deposits in Layered Intrusions Descriptive Model for Reef-Type PGE and Contact-Type Cu-Ni-PGE Deposits.pdf
04/23/2020 05:35 AM 1,501,060 Magmatic_Ni-Cu-_PGE_deposits_in_magma.pdf
03/10/2016 09:10 AM 22,072,057 metallogeny-of-ultramafic-PGE.pdf
02/25/2011 03:29 PM 470,926 Method for treatment of engine exhaust gases.pdf
10/03/2019 05:20 AM 1,011,222 Mineralogy_and_geochemistry_of_platinum-.pdf
04/04/2020 05:50 AM 1,127,671 Mineralogy_composition_and_PGM_of_chromites in Greece.pdf
03/13/2012 03:51 AM 245,049 of881(A new platinum-group-element discovery at Crescent Peak).pdf
10/03/2019 05:20 AM 1,252,468 ON_THE_ASSOCIATION_OF_PALLADIUM-BEARING.pdf
03/08/2020 07:09 AM 996,942 On_the_Origin_of_Platinum-Group_Element-.pdf
02/01/2020 11:55 PM 1,894,493 ON_THE_ORIGIN_OF_THE_PGE_MINERALIZATION.pdf
12/20/2010 02:26 PM 149,861 Palladium sortion using chitosan derivatives.pdf
03/03/2016 02:45 AM 1,207,485 PALLADIUM-BEARING GOLD.pdf
12/24/2010 12:36 PM 57,872 palladium.pdf
10/03/2019 05:20 AM 879,434 PALLADIUM_AND_PLATINUM_MINERALS_FROM_THE.pdf
02/01/2020 11:55 PM 3,052,378 Partial_Melting_Processes_and_Cu-Ni-PGE.pdf
11/28/2019 03:31 AM 8,895,340 Petrogenesis of the Platinum-Group Minerals.pdf
11/28/2019 03:31 AM 1,105,880 PGE-Adapted-227-232_ELEM_V4n4.pdf
03/03/2016 07:52 AM 1,096,384 PGE-bearing mineral locations.pdf
12/13/2019 04:50 PM 429,344 PGM_Guide_Questions and Answers.pdf
12/13/2019 04:50 PM 7,509,623 pgm_market_report_may_19.pdf
12/15/2011 03:08 AM 12,466 PGM_Uses.pdf
06/15/2018 05:28 AM 862,735 Platinum Group Element Deposits 2.pdf
03/16/2016 10:54 PM 683,280 Platinum Group Element Deposits.pdf
01/23/2019 12:16 AM 3,408,768 Platinum Group Element, Chromium, and Vanadium Deposits.pdf
07/17/2018 11:49 PM 1,932,021 Platinum Group Tellurides.pdf
12/24/2019 07:38 PM 979,760 PLATINUM IN OREGON.pdf
05/19/2020 11:58 AM 29,201,426 Platinum-Group Elements in Magnetic Concentrates.pdf
11/28/2019 03:30 AM 1,586,684 PLATINUM-GROUP MINERALS AND OTHER DETRITAL COMPONENTS.pdf
01/09/2020 02:58 PM 38,925,845 Platinum-group_elemental_chemistry_of_Fe_Ti_oxide bearing gabbroic intrusions.pdf
02/01/2020 11:55 PM 6,530,594 Platinum-group_elements_PGE_in_various_geotectonic settings.pdf
04/04/2020 05:50 AM 903,720 Platinum-group_element_mineralogy_and geochemistry of chromitite, Russia.pdf
01/16/2020 07:25 PM 899,196 Platinum-group_element_potential_of_porp.pdf
03/08/2020 07:09 AM 796,341 Platinum-Group_Mineral_Characterization.pdf
03/23/2016 04:02 AM 1,059,478 PLATINUM-METAL MINERALS.pdf
07/17/2018 11:31 PM 731,926 Platinum-Tellurides.pdf
12/24/2010 12:37 PM 61,090 platinum.pdf
12/25/2011 10:15 PM 14,966 PlatinumPalladiumSeparationMethod.pdf
03/08/2020 07:09 AM 49,877,271 Platinum_Group_Elements_PGE_geochemistry.pdf
02/28/2020 02:52 AM 651,639 Platinum_Group_Mineral_Characterization.pdf
04/27/2020 06:11 AM 154,409 platinum_in_arizona.pdf
07/17/2018 09:37 PM 720,703 Platinum_Occurances.pdf
10/03/2019 05:20 AM 1,239,564 PLATINUM_PALLADIUM_NUGGETS_AND_MERCURY-R.pdf
12/13/2019 04:50 PM 247,608 pmr-v12-i3-086-088.pdf
12/13/2019 04:50 PM 508,856 Press Release December 2017_IPA PGM Guide.pdf
04/04/2020 05:50 AM 1,163,842 Pt_Fe_NUGGETS_DERIVED_FROM clinopyroxenitedunite massifs, Russia.pdf
08/14/2020 04:41 AM 11,809,916 Recovery of Platinum Group Metals from Spent Furnace Linings and Used Automotive Catalysts.pdf
04/05/2016 09:14 PM 274,374 Rhenium variations in molybdenite.pdf
01/24/2019 12:21 PM 483,152 Rhenium.pdf
01/30/2019 09:08 PM 932,316 Ruthenian pyrite in Chromium Layer.pdf
12/16/2019 10:23 AM 1,732,136 SGS MIN TP2002 03 Beneficiation and Extractive Metallurgy of PGE.pdf
03/17/2016 12:37 AM 1,381,640 SGS MIN TP2006 06 Recovery of Cu Ni Co Zn Pd Pt Au at NorthMet Deposit.pdf
10/17/2019 11:46 PM 978,831 Skaergaard Intrusion, Greenland.pdf
03/16/2016 10:51 PM 5,527,164 Sorption of the Platinum-group elements.pdf
08/26/2020 07:23 AM 4,709,669 Source and Bedrock Distribution of Gold and Platinum-Group Metals in the Slate Creek Area, Northern.Chistochina Mining District, East-Central Alaska.pdf
04/04/2020 05:50 AM 10,300,033 Stratiform_platinum-group_element_mineralization in the layered Northern Ultramafic Center of the Lac des Iles Intrusive Complex Canada.pdf
10/17/2019 11:46 PM 384,117 Sulfur Isotope Studies of the Stillwater Complex.pdf
 
03/26/2016 11:49 PM 189,215 Flotation of mixed copper oxide.pdf
08/31/2020 12:36 AM 26,509,907 Flotation Reagents Applied Surface Chemitry on Minerals Flotation and Energy Resources Beneficiation Volume 1 Functional Principle by Dianzuo Wang.pdf
08/31/2020 12:36 AM 14,069,028 Flotation Reagents Applied Surface Chemistry on Minerals Flotation and Energy Resources Beneficiation Volume 2 Applications by Dianzuo Wang.pdf
08/31/2020 12:36 AM 5,184,888 Flotation Technology Volume 12 by Nazih K. Shammas PhD, Gary F. Bennett PhD (auth.), Lawrence K. Wang, Nazih K. Shammas, William A. Selke, Donald B. Aulenbach.pdf
03/29/2016 11:01 PM 19,820,205 Flotation Tests of Idaho Ores.pdf
03/23/2016 11:07 PM 675,532 Flotation_Fundamentals.pdf
08/07/2020 07:20 AM 34,312,072 Froth flotation a century of innovation by Maurice C Fuerstenau Graeme J Jameson R H Yoon (z-lib.org).pdf
08/02/2020 09:13 AM 1,667,094 Handbook of Flotation Reagents Chemistry, Theory and Practice Volume 2 Flotation of Gold, PGM and Oxide Minerals by Srdjan M. Bulatovic (z-lib.org).pdf
03/23/2016 10:18 PM 374,215 Makanza_Flotation(2008).pdf
03/23/2016 11:01 PM 457,340 OnTheFloatabilityOfGoldGrains.pdf
03/23/2016 11:05 PM 97,581 Pyrite-Gold Recovery in Copper Rougher Flotation.pdf
09/18/2020 06:35 AM 5,675,527 Sulphide_mineral_flotation_a_new_insight.pdf
08/31/2020 12:35 AM 37,963,205 Surface Chemistry of Froth Flotation Volume 1 Fundamentals by S. Ramachandra Rao.pdf
12/30/2010 06:52 PM 304,001 4_Thermophilic_Heap_Leaching.pdf
12/20/2010 02:29 PM 570,611 A processing method of the goldsmith's and electronic Au-Ag-containing wastes.pdf
12/24/2010 08:01 AM 741,962 AssayingOres,Concentrates,andBullion.pdf
02/25/2011 08:31 PM 58,698 Au_Reactions.jpg
12/20/2010 02:02 PM 330,603 BDG_Full_Process.pdf
12/25/2010 01:29 AM 70,566 bromine leaching - 1990s research in Indiana.pdf
12/23/2010 03:05 PM 837,968 CAUSTIC-SIDE SOLVENT-EXTRACTION MODELING FOR HANFORD INTERIM PRETREATMENT SYSTEM.pdf
01/01/2011 06:59 PM 1,117,202 Chapter 2 Overview of Mining and Mineral Processing Operations.pdf
11/12/2006 11:02 AM 6,385,534 Chemical metallurgy.pdf
02/24/2020 05:19 AM 6,385,534 Chiranjib_Kumar_Gupta_Chemical_Metallurg.pdf
11/28/2019 09:21 AM 1,081,986 Chlorine Dioxide.pdf
12/23/2010 02:54 PM 1,647,380 Decomposing Ammonium Sulfate.pdf
02/25/2011 03:32 PM 207,228 Desensitized free-flowing red phosphorus.pdf
12/15/2010 08:48 AM 473,255 Detection and Characterization of Threat Material.pdf
12/15/2010 08:42 AM 289,276 ECONOMICAL Recovery of By-Products in the Mining Industry.pdf
10/26/2009 10:10 PM 16,272,853 Electrochemical_Dictionary.pdf
12/28/2010 05:38 AM 15,998,670 Electrochemistry_of_Flotation_of_Sulphide_Minerals.pdf
07/23/2010 10:12 PM 111,266,996 Encyclopedia of Separation Science.pdf
10/26/2009 10:06 PM 33,370,236 Fire_and_Explosion_Hazards_Handbook_of_Industrial_Chemicals.pdf
08/16/2023 07:03 AM 146,304 Frontiers in Gold Chemistry.pdf
01/07/2011 06:06 PM 4,197,846 G090301_Matthew.pdf
12/30/2010 06:54 PM 6,106,806 Heap Leaching.pdf
01/06/2011 07:52 AM 14,787,137 Horton_References.pdf
01/01/2011 10:19 AM 6,488,999 How to refine a A B-61 nuclear bomb.pdf
12/15/2010 08:27 AM 842,353 Hydrometallurgy.pdf
12/25/2010 01:10 AM 851,398 Hydrometallurgy2.pdf
12/25/2010 01:32 AM 61,608 iGoli chlorine leaching - 2000s research in South Africa.pdf
09/02/2020 02:18 AM 16,009,652 Inorganic Chemistry in Focus III by Gerd Meyer, Dieter Naumann, Lars Wesemann (z-lib.org).pdf
12/30/2010 06:07 PM 13,368 Inorganic Leaching Science.pdf
09/01/2020 06:08 AM 2,317,127 InTech-Corrosive_effects_of_chlorides_on_metals.pdf
03/15/2011 04:35 AM 236,756 iodinmyb02r.pdf
12/15/2010 08:56 AM 1,396,802 lehne_ore_dressing_2006.pdf
12/15/2010 08:33 AM 1,134,205 meetings_hydrometallurgy_2008_robert_shoemaker.pdf
03/31/2011 06:20 AM 105,972 Metal_dissolution_process.pdf
12/30/2010 06:05 PM 1,014,834 Microbial Leaching of Metals.pdf
01/24/2011 04:21 AM 9,020,378 Modern Physical Metallurgy and Materials Engineering.pdf
12/30/2010 04:28 PM 180,129 nitric acid azeotrop.pdf
12/23/2010 03:03 PM 2,550,913 Novel Binders and Methods for Agglomeration of Ore.pdf
12/23/2010 03:03 PM 808,557 NOVEL
12/23/2010 03:03 PM 808,557 NOVEL IN-SITU METAL AND MINERAL EXTRACTION TECHNOLOGY.pdf
02/25/2011 01:01 PM 488,572 NOx.pdf
12/23/2010 12:14 AM 605,761 Nuclear Techniques for Ore Grade Estimation.pdf
01/24/2011 04:35 AM 6,356,719 Physical Metallurgy and Advanced Materials.pdf
12/23/2010 03:15 PM 584,968 Recovery of Minerals and Metals from Geothermal Fluids.pdf
01/31/2011 10:29 AM 848,696 Recovery-of-Precious-Metals-From-Electronic-Waste.pdf
01/10/2011 01:33 PM 2,137,253 Refining Precious Metal Wastes C[1][1].MHoke.pdf
10/26/2009 10:26 PM 27,237,091 Rules_Of_Thumb_For_Chemical_Engineers,_3rd_Edition.pdf
12/28/2010 11:39 AM 6,453,600 Studies in the hydrometallurgy of mercury sulfide ores.pdf
12/20/2010 02:27 PM 151,347 Sulfuric acid.pdf
02/05/2011 11:56 AM 148,139 Sulfur_Dioxide-English.pdf
01/01/2011 06:57 PM 295,714 SUSTAINABLE RECOVERY OF BY-PRODUCTS IN THE MINING INDUSTRY .pdf
12/15/2010 08:33 AM 250,873 Teaching and Learning Adaptive Hydrometallurgy-Final edition.pdf
12/23/2010 03:10 PM 11,996,302 THE CHEMISTRY AND METALLURGY OF MISCELLANEOUS MATERIALS.pdf
12/23/2010 03:11 PM 1,282,098 The Decontamination and Recovery of Precious Metals.pdf
12/23/2010 03:22 PM 2,539,428 THE WEATHERING OF A SULFIDE OREBODY--SPECIATION AND FATE OF SOME POTENTIAL CONTAMINANTS.pdf
08/16/2023 07:01 AM 506,176 Theoretical chemistry of gold III.pdf
01/08/2011 07:54 PM 88,495,309 The_Encyclopedia_Americana.pdf
12/07/2019 07:37 AM 605,301 Timet-Metallurgists-101912.pdf
12/25/2010 01:31 AM 71,161 tincture of iodine leaching - 2000s research in Japan.pdf
01/28/2011 11:12 AM 608,745 TOC plus samples.pdf
12/20/2010 02:55 PM 60,038,643 Unit Processes in Extractive Metallurgy - Hydrometallurgy.pdf
12/30/2010 06:47 PM 2,660,061 USBMIC8945Agglomeration-HeapLeachingOperationsinthePreciousMetalsIndustry.pdf
12/20/2010 02:05 PM 938,706 vol2_issue5.pdf
11/04/2007 12:11 AM 42,069,946 Wills' Mineral Processing Technology, Elsevier (2005), 0750644508.pdf
11/15/2014 09:28 AM 1,309,426 1998_Assessment_of_Undiscovered_Deposits.pdf
03/10/2016 09:27 AM 364,850 Ag-Au-S_deposits.pdf
12/23/2010 12:21 AM 890,811 Arsenate and Arsenite Sorption on Carbonate Hosted Precious Metals Ore.pdf
03/10/2016 09:02 AM 10,306,885 carbonate-hosted-deposits.pdf
01/31/2019 04:17 AM 107,350 carbonatite deposit report.pdf
01/28/2019 08:45 AM 1,283,220 Changes in Ore Deposits - 1924.pdf
01/30/2019 09:08 PM 1,623,666 COLLOFORM AND FRAMBOIDAL PYRITE.pdf
07/30/2018 02:04 AM 8,522,841 Craig_Vaughan_IGNEOUS ORE MINERAL ASSEMBLAGES_Chptr_09.pdf
03/26/2016 10:13 PM 8,510,062 CU, AU, AND ZN-PB SKARN DEPOSITS.pdf
03/23/2016 04:45 AM 1,356,972 CUPRIFEROUS AND NICKELIFEROUS PYRRHOTITE.pdf
04/30/2020 02:02 PM 586,791 DATABASE OF SIGNIFICANT DEPOSITS OF GOLD, SILVER, COPPER, LEAD, AND ZINC.pdf
01/01/2011 07:06 PM 182,571 DNT_Precious_Metals_precious_wilderness.pdf
01/21/2020 02:57 PM 5,589,290 e-book_metals_report2_recycling_130920.pdf
03/17/2016 12:37 AM 7,352,886 Evaluation-of-Metallic-Mineral-Resources.pdf
05/11/2020 04:54 PM 557,067 Experiments with colloidal gold and silver.pdf
03/16/2016 11:33 PM 67,994 Fe Skarn Deposits.pdf
03/31/2016 05:25 PM 2,180,980 Geochemistry of Carbonate Sediments and Sedimentary Carbonate Rocks.pdf
08/20/2012 07:48 PM 42,045,800 geographical and geological occurrence of the precious metals with their mineralogical associations.pdf
03/16/2016 11:55 PM 97,609 Geology of Ore Deposites .pdf
03/17/2016 12:06 AM 12,822,648 GOSSANS.pdf
10/03/2019 05:20 AM 957,287 HONGSHIITE_PtCu_FROM_ITABIRITE-HOSTED_Au.pdf
08/27/2020 01:36 PM 22,673,099 Hydrothermal Iron Oxide Copper-Gold and Related Deposits A Global Perspective - Advances in the Understanding of IOCG Deposits - Volume 3 by T.M. Porter (editor) (z-lib.org).pdf
03/10/2016 09:58 AM 367,055 igneous-related FE deposits_IOCG.pdf
03/10/2016 09:34 AM 2,343,632 igneous-related metallogeny.pdf
03/26/2016 11:38 PM 2,964,890 INTRUSION-RELATED POLYMETALLIC CARBONATE DEPOSITS.pdf
01/27/2019 11:22 PM 1,413,416 INVESTIGATIONS OF GOSSANS.pdf
03/16/2016 11:12 PM 461,903 KUPFERSCHIEFER TYPE DEPOSIT.pdf
03/30/2016 01:56 AM 30,546,952 Lead Materials Survey.pdf
06/15/2018 02:59 PM 5,052,779 Lead-Zinc Gossans.pdf
03/29/2016 11:56 PM 138,926,644 Microscopic Structure and Concentratability of the Important Iron Ores.pdf
03/16/2016 11:59 PM 1,227,482 Mineral Deposit Models.pdf
03/16/2016 09:45 PM 6,832,121 Mineralization Styles & Metal Zonation.pdf
01/28/2019 12:00 AM 7,969,133 mineralogical and analytical information.pdf
03/16/2016 07:13 PM 583,242 mineralogy of the antimony oxides and antimonates.pdf
07/30/2018 02:21 AM 33,728,099 Mineral_Deposits_chpt06.pdf
01/30/2019 09:08 PM 688,995 MORPHOLOGY OF PYRITE.pdf
03/17/2016 02:35 AM 2,063,072 pb ores and metallogenic terranes.pdf
10/03/2019 05:20 AM 1,631,442 Persistence_of_mantle_lithospheric_Re-Os.pdf
07/18/2018 05:17 AM 498,867 Phosphate-Minerals-in-Oxidized-ore-bodies.pdf
03/31/2016 06:29 PM 20,099,808 Physical properties of evaporite minerals.pdf
07/18/2018 06:46 PM 2,453,027 placer-deposits-and-their-geology.pdf
03/20/2016 01:48 PM 5,333,089 Polymetallic Vein and Replacement Deposits-part2.pdf
03/16/2016 11:33 PM 1,043,341 Polymetallic Vein and Replacement Deposits.pdf
11/01/2020 05:02 PM 520,041 PRECIOUS METALS IN COPPER SMELTING.pdf
01/28/2019 09:16 AM 1,611,630 precious metals in minerals.pdf
11/15/2014 11:02 AM 4,496,353 Principles_of_geochemical_prospecting.pdf
03/16/2016 11:12 PM 7,803,106 SHDG deposits.pdf
04/04/2020 05:50 AM 46,864,987 Silver_and_Gold-1873-Metallurgy and Mining Industry.pdf
03/26/2016 11:37 PM 481,285 SKARN AND POLYMETALLIC DEPOSITS.pdf
07/28/2018 11:58 AM 440,664 Skarn formations.pdf
03/27/2016 03:28 AM 1,671,297 SUPERGENE ALTERATION OF URANIUM-BEARING VEINS.pdf
07/30/2018 02:19 AM 310,893 Supergene Ore and Gangue Characteristics.pdf
04/14/2016 12:50 PM 19,180,753 0The Metallurgy Of Gold By M Eissler.pdf
01/29/2019 08:42 PM 2,894,578 2011 Porphyry Cu-Au-Mo-epithermal Ag-Pb-Zn-distal hydrothermal Au deposits- A linked ore system.pdf
08/13/2016 03:29 AM 13,395,111 40_06(Gold-Bearing Gravels).pdf
04/16/2020 12:32 AM 233,048 8-or-colloidal.pdf
09/07/2020 02:03 PM 917,876 ADSORPTION OF GOLD FROM Au(III)-CHLORIDE SOLUTIONS ON ALTERNATIVE MATERIALS TO ACTIVATED CARBON INORGANIC MATERIALS by T. Feldmann ,G.P. Demopoulos (z-lib.org).pdf
03/10/2016 09:27 AM 364,850 Ag-Au-S_deposits.pdf
04/07/2020 10:20 PM 2,214,841 An unusual mesothermal gold-silver deposit.pdf
01/30/2019 02:55 PM 13,468,876 Archaean lode-gold deposits.pdf
01/30/2019 02:54 PM 5,199,229 Archaen Lode-gold hydrothermal deposits.pdf
01/27/2019 11:59 PM 33,379,699 Archean Gold Deposit Survey S. Africa.pdf
04/07/2020 10:20 PM 5,199,229 Archean Lode-gold deposits.pdf
06/15/2018 10:51 AM 357,818 ARCHEAN LOW-SULFIDE Au-QUARTZ VEINS.PDF
01/30/2019 02:55 PM 4,364,657 Archean orogenic lode gold.pdf
07/26/2020 08:24 AM 1,207,485 ASSOCIATION OF PALLADIUM-BEARING GOLD, HEMATITE AND GYPSUM.pdf
03/16/2016 11:32 PM 41,841 Au in Iron Formations.pdf
04/07/2020 10:20 PM 166,506 AVALON DEVELOPMENT CORPORATION-2015-PGM-GOLD-TECHREPORT.pdf
07/30/2018 05:23 AM 2,758,124 Banded Iron Formation and Gold Mineralization.pdf
08/26/2020 07:23 AM 10,538,315 Banded iron formations, pyritic black shale, and gold deposits.pdf
09/20/2019 10:36 AM 4,541,934 Biogenicity of gold- and silver-bearing siliceous sinters.pdf
04/07/2020 10:20 PM 304,753 CHARACTERISTICS OF GOLD DEPOSITS IN NORTHERN SONORA, MEXICO.pdf
04/07/2020 10:20 PM 4,271,153 Colloidal Processes in the Formation of Bonanza-Grade Gold Ores.pdf
01/10/2021 06:19 AM 1,027,146 Colored Gold Alloys.pdf
04/07/2020 10:20 PM 3,792,252 Controls on Syenite-Hosted Gold Mineralization.pdf
04/07/2020 10:20 PM 689,286 copper-gold mineralization-Yukon.pdf
03/20/2016 05:50 AM 850,908 Description and grades and tonnages of gold-bearing skarns.pdf
02/19/2019 07:20 PM 8,390,054 Development of a process selection method for gold ores using case-based reasoning.pdf
07/25/2020 02:17 AM 14,361,606 Different Skarn Metallogenesis between the Giant Beiya Au and Machangqing Cu-Mo-(Au) Deposits in Yunnan, SW China.pdf
03/23/2016 06:47 AM 668,061 disseminated gold deposits.pdf
03/17/2016 05:48 AM 688,392 DISSOLUTION OF GOLD.pdf
07/26/2020 08:24 AM 3,321,029 Effective Gold Recovery from Near-Surface Oxide Zone Using Reductive Microwave Roasting and Magnetic Separation.pdf
04/22/2020 02:21 PM 3,484,797 EPA-EXTRACTION AND BENEFICIATION OF ORES AND MINERALS- VOL. 2- GOLD.pdf
08/16/2020 01:40 AM 357,296 EPA-GOLD AND SILVER.pdf
07/30/2018 02:25 AM 27,681,732 epigenetic gold occurrances.pdf
03/03/2016 05:44 PM 1,511,392 EPITHERMAL GOLD FOR EXPLORATIONISTS.pdf
03/03/2016 05:30 PM 416,675 EPITHERMAL QUARTZ-ALUNITE AU DEPOSITS.pdf
08/26/2020 07:23 AM 11,985,457 GEOCHEMICAL DISPERSION RELATED TO GOLD MINERALIZATION, WESTERN AUSTRALIA.pdf
12/28/2010 08:15 AM 4,286,223 Geodynamic settings and tectonic model of skarn gold deposits.pdf
07/25/2020 02:17 AM 1,105,158 Geologic Characteristics of Sediment-and Volcanic-Hosted Disseminated Gold Deposits-Publications Listing.pdf
04/07/2020 10:20 PM 115,303 GNEISS-HOSTED KYANITE GOLD AND GNEISS HOSTED EPITHERMAL GOLD.pdf
09/15/2011 06:48 PM 1,777,897 gold (1).pdf
07/26/2020 09:08 AM 7,818,687 GOLD - MOLYBDENUM METALLOGENY-CHINA.pdf
02/19/2019 07:21 PM 53,205,486 GOLD -ITS GEOLOGICAL OCCURRENCE AND GEOGRAPHICAL DISTRIBUTION.pdf
07/26/2020 08:24 AM 3,012,742 GOLD AND COPPER DEPOSITS NEAR PAYSON, ARIZONA.pdf
09/20/2019 10:37 AM 7,014,822 Gold and Other Minor Elements Associated with the Hot Springs and Geysers of Yellowstone.pdf
10/06/2019 01:41 AM 2,381,600 Gold Bearing Slates of Novia Scotia.pdf
04/07/2020 10:20 PM 737,658 Gold Deposits and Their Geological Classification.pdf
03/10/2016 08:12 AM 1,357,503 GOLD DEPOSITS IN THE UNITED STATES.pdf
01/27/2019 11:59 PM 888,744 GOLD DEPOSITS-NOVA SCOTIA.pdf
12/25/2010 02:17 AM 161,083 Gold extraction by chlorination using a pyrometallurgical process.pdf
05/11/2020 05:07 PM 1,772,513 Gold from the Assyrian Colony Period.pdf
06/15/2018 09:34 AM 3,486,514 Gold in Greenstone Belts.pdf
03/23/2016 10:38 AM 875,320 gold in limonite.pdf
03/23/2016 01:13 AM 1,646,194 GOLD IN MASSIVE SULFIDES.pdf
04/07/2020 10:20 PM 188,663 Gold in Metamorphic rocks_ Facts and Fancy.pdf
01/31/2023 09:46 AM 1,848,818 Gold in Minerals and the Composition of Native Gold.pdf
07/17/2018 11:57 PM 1,848,818 Gold in Minerals.pdf
03/20/2016 05:45 AM 3,223,107 Gold in Porphyry Copper Systems.pdf
04/07/2020 10:20 PM 1,042,425 GOLD MINERALIZATION IN GRANITOIDS.pdf
04/07/2020 10:20 PM 2,625,485 Gold mineralization in the Ourika Gneiss-2014.pdf
06/15/2020 06:40 AM 11,296,148 Gold Mining in the Carolinas.pdf
03/19/2011 10:07 AM 91,400 Gold recovery with I2 1.pdf
03/19/2011 10:08 AM 423,745 Gold recovery with I2 2.pdf
03/19/2011 10:08 AM 83,710 Gold recovery with I2 3.pdf
03/19/2011 10:07 AM 472,423 Gold recovery with I2 and diacetone alcohol.pdf
01/10/2011 01:31 PM 2,878,743 GOLD REFINING FORUM HANBOOK VOL 1.pdf
01/31/2023 09:45 AM 250,103 Gold that We do not Recognise.pdf
09/15/2011 06:41 PM 32,679 Gold Uses.pdf
08/14/2020 04:41 AM 3,080,268 Gold _ The most precious of metals (Part2).mhtml
01/31/2019 04:17 AM 312,269 GOLD-ANTIMONY DEPOSITS report.pdf
03/03/2016 05:31 AM 495,046 gold-bearing arsenian pyrite.pdf
03/20/2016 01:41 PM 2,786,975 Gold-bearing Polymetallic Veins and Deposits-part1.pdf
08/13/2016 03:24 AM 5,084,267 Gold-Bearing-ancient-rivers-cal.pdf
08/13/2016 03:29 AM 50,717,319 Gold-Bearing-ancient-rivers-yuba-cal.pdf
03/23/2016 12:56 AM 469,740 Gold-in-pyrite-barker-Econ-Geol-2009.pdf
01/14/2011 09:55 AM 2,350,140 Gold-NevadaBureauMinesGeology.pdf
06/15/2018 09:58 AM 2,025,575 GOLD-RICH BANDED IRON FORMATIONS.pdf
03/03/2016 02:57 AM 645,577 gold-skarn.pdf
09/15/2011 06:48 PM 140,771 gold.pdf
03/23/2016 06:51 AM 2,347,688 Golden Butte sediment-hosted disseminated (Carlin-type) gold deposit.pdf
04/08/2016 07:07 PM 2,741,585 GoldMercury1982.pdf
05/12/2020 12:55 AM 737,658 Gold_Deposits_and_Their_Geological_Classification.pdf
03/16/2016 10:14 PM 218,893 gold_platinum_report.pdf
01/27/2019 11:59 PM 1,206,923 Gossan Refractory gold and silver ore.pdf
04/07/2020 10:20 PM 1,371,608 Greenstone_gold_exploration.pdf
04/08/2016 07:25 PM 4,476,513 Guide-to-Epithermal-Gold-Deposits.pdf
03/03/2016 05:26 PM 3,898,044 High-Sulfidation Epithermal Pyrite-Hosted Au (Ag-Cu) Ore Formation.pdf
02/19/2019 07:21 PM 1,970,590 Introduction to Geology and Resources of Gold, and Geochemistry of Gold.pdf
08/16/2023 06:49 AM 747,716 Invisible Gold.pdf
02/19/2019 07:21 PM 11,492,999 Iron Oxide Copper-Gold Deposits Geology, Space-Time Distribution, and Possible Modes of Origin.pdf
06/15/2018 10:03 AM 1,356,751 Iron Oxide-Copper-Gold Deposits in Finland.pdf
04/07/2020 10:20 PM 14,060,356 Late Jurassic Fault-Hosted Gold Mineralization.pdf
04/07/2020 10:20 PM 1,242,118 lode gold deposits in a Mesoarchean greenstone belt.pdf
04/07/2020 10:20 PM 16,013,660 LOGE GOLD.pdf
01/30/2019 02:54 PM 354,944 magmatic model for the origin of Archean Au-quartz vein ore systems.pdf
04/19/2019 01:49 AM 1,622,572 Map showing locations of epithermal gold-silver deposits.pdf
01/02/2012 07:16 PM 1,836,504 mercury and gold in the drylakes of Nevada.pdf
03/10/2016 09:13 AM 38,268,154 mesothermal-epithermal-gold-deposits.pdf
03/22/2016 11:50 PM 44,733,634 metallurgyofgold00roserich.pdf
03/23/2016 01:18 AM 5,969,965 metaturbidite-hosted mesothermal gold deposits.pdf
01/31/2019 04:17 AM 2,930,134 Mineral Commodity Profiles-Gold.pdf
01/30/2019 02:54 PM 18,982,982 Mineralogy of S. African Epitherrmal Gold Ores.pdf
 
03/30/2016 02:21 AM 17,559,473 The Principles and Practice of Sampling Metallic Metallurgical Materials, with Special Reference to the Sampling of Copper Bullion.pdf
11/15/2014 09:14 AM 20,311,183 The Theory and Process of Ore Dressing.pdf
03/30/2016 03:44 AM 2,442,017 The Use of a Centrifugal Contactor for Component Concentration by Solvent Extraction.pdf
03/30/2016 02:25 AM 40,651,900 Thermodynamic Properties of 65 Elements, Their Oxides, Halides, Carbides and Nitrides.pdf
03/31/2016 06:28 PM 8,325,663 Thermodynamic properties of minerals.pdf
01/02/2020 02:59 AM 117,990 Titanium Anode Basket Application Note.pdf
03/29/2016 10:36 PM 2,421,965 TREATMENT OF CYANIDE SOLUTIONS AND SLURRIES USING AIR-SPARGED HYDROCYCLONE (ASH) TECHNOLOGY.pdf
03/30/2016 02:18 AM 23,664,085 Treatment of Manganese-Silver Ores.pdf
01/02/2020 09:07 PM 7,185,989 Trends in Hydrometallurgy.pdf
03/23/2016 10:19 PM 299,213 Ultra Fine Grinding - A Practical Alternative to Oxidative.pdf
02/13/2020 12:05 PM 5,060,468 Understanding Mineral Liberation during Crushing.pdf
04/24/2012 04:54 PM 616,525 urn009853.pdf
03/23/2012 11:25 PM 3,198,531 USBMIC8969GoldAndSilverLeaching.pdf
01/02/2020 09:06 PM 1,493,584 USE OF HYDROMETALLURGY IN DIRECT PROCESSING OF BASE METAL-PGM CONCENTRATES.pdf
10/09/2019 02:07 AM 2,523,666 VAT_LEACHING_AND_ELUTION_PLANT_-_GOLD_PROCESSING.docx
01/02/2020 02:59 AM 3,439,804 WPJ7_75_Fine_Gold_Recovery_Methods.pdf
08/20/2012 05:50 PM 2,866,401 You_Can_Smelt_Too.pdf
06/28/2014 07:27 AM 2,471,728 0C. M. Hoke Refining Precious Metal Wastes.pdf
07/11/2017 11:06 PM 19,789,336 0textbook of fire assaying bugbrich.pdf
02/04/2012 06:07 PM 777,643 29035575-Peroxide-Acid-Method.pdf
03/15/2011 12:39 PM 4,889,339 31943389-Gold-Iodine-Carbon.pdf
08/13/2016 03:34 AM 11,985,368 40_10(Fire Assay of Gold and Silver).pdf
02/04/2012 06:14 PM 4,680,479 41281820-Gold-Chemistry.pdf
10/02/2020 12:44 AM 1,372,412 442 - CHOKO TEREZA ITO_TADAHISA NISHIMURA_KASUTERU TOZAWA - BEHAVIOR OF ANTIMONY AND ARSENIC IN SULFURIC ACID SOLUTION.pdf
02/04/2012 06:24 PM 2,008,167 65238247-Chgex-Leaching.pdf
12/15/2010 05:00 AM 4,534,564 75_Gold_Recovery_Methods.pdf
01/23/2020 11:20 PM 349,880 A HISTORY OF MINERAL CONCENTRATION - MINE TAILINGS.pdf
08/16/2023 07:09 AM 10,128,851 A Manual on Fire Assaying.pdf
01/02/2020 09:07 PM 1,091,421 A Process for the Separation of Noble Metals By Solvant Extraction.pdf
08/16/2023 06:55 AM 161,696 Advances in Mineral Processing and Hydrometallurgy.pdf
03/29/2016 08:55 PM 11,854,233 Agglomeration and Leaching of Slimes andOther Finely Divided Copper Ores.pdf
02/25/2011 01:20 PM 334,842 Ammonia extraction of gold and silver from ores and other materials.pdf
05/04/2016 05:16 AM 150,696 Ammoniacal thiosulphate leaching of gold ore.pdf
03/30/2016 12:25 AM 82,172,450 Analytical Methods for Certain Metals Including Cerium, Thorium, Molybdenum, Tungsten, Radium, Uranium, Vanadium, Titanium and Zirconium.pdf
03/23/2016 03:47 AM 4,271,391 ANALYTICAL METHODS FOR DETERMINING GOLD.pdf
10/09/2019 02:07 AM 178,472 Application_of_Alternative_Lixiviants_for Secondary Heap Leaching of Gold.pdf
03/30/2016 03:21 AM 42,288,360 Appraisal of Minerals Availability for 34 Commodities.pdf
09/15/2011 07:17 PM 285,629 Article_Cardarelli_Gold_Leaching.pdf
02/20/2020 01:31 PM 3,177,289 Aseismic Refinement of Orogenic Gold Systems.pdf
08/12/2020 08:28 AM 26,839,068 ASSAYING AND SMELTING NOBLE METALS IN SIXTEENTH-CENTURY AUSTRIA.pdf
08/26/2012 10:20 AM 5,797,060 A_manual_of_fire_assaying.pdf
12/27/2010 08:08 PM 24,247,877 A_textbook_on_metallurgy_of_gold_silver.pdf
11/15/2014 08:51 AM 27,433,791 A_text_book_of_ore_dressing.pdf
03/23/2016 03:43 AM 19,858,870 BALKAN MINERAL PROCESSING CONGRESS.pdf
06/15/2020 12:08 PM 112,008 borates-metallurgical-applications.pdf
03/24/2016 12:02 AM 2,636,883 Borax Method of Gold Extraction.pdf
08/21/2020 09:05 PM 17,219,220 Cablebolting in Underground Mines by Hutchinson Diederichs (z-lib.org).pdf
03/29/2016 05:36 PM 17,693,487 Center for Advanced Separation Technology-Report.pdf
03/23/2016 04:15 AM 16,644,050 Chemical Analysis.pdf
03/29/2016 10:55 PM 1,927,722 chemistry and migration behavior of actinides and fission products.pdf
08/11/2020 08:45 PM 6,385,534 Chiranjib_Kumar_Gupta_Chemical_Metallurg.pdf
12/25/2010 02:19 AM 102,810 Chlorine Hydrometallurgical Process for Gold Recovery(Amberlite XAD-7).pdf
12/25/2010 01:32 AM 82,479 chlorine leaching - dissolving gold.pdf
05/29/2012 11:29 PM 263,591 cls20.pdf
05/29/2012 11:30 PM 232,284 cls25 revised.pdf
03/23/2012 11:27 PM 335,203 Co-intensification of gold leaching with heavy metals and hydrogen peroxide.pdf
08/01/2020 04:01 AM 401,133 Coke Ovens.pdf
02/04/2019 09:56 AM 266,862 Controlling Melt Loss when Melting Gold Alloys.pdf
04/23/2020 05:35 AM 492,176 Copper Heap leaching and BRISA process.pdf
03/30/2016 02:24 AM 21,237,728 Copper Leaching Practices in the Western United States.pdf
12/15/2011 03:12 AM 213,947 CuCl.pdf
03/23/2016 04:45 AM 1,356,972 CUPRIFEROUS AND NICKELIFEROUS PYRRHOTITE.pdf
03/29/2016 04:22 AM 63,851,579 Cyanide_Practice_1910_to_1913.pdf
03/29/2016 10:53 PM 46,729,670 Data on Theoretical Metallurgy.pdf
03/23/2016 11:08 PM 961,696 Desulpherization-of-mine-tailings.PDF
03/03/2016 03:21 AM 1,206,923 diagnostic leaching.pdf
03/30/2016 03:09 AM 43,207,574 DISPOSAL OF FLUIDIZED-BED COMBUSTION ASH IN AN UNDERGROUND MINE TO CONTROL ACID MINE DRAINAGE AND SUBSIDENCE.pdf
01/02/2020 09:07 PM 1,611,630 distribution of trace precious metals in minerals.pdf
08/01/2020 04:01 AM 581,986 Effect of coke reactivity and nut coke on blast furnace operation.pdf
09/15/2020 11:48 AM 20,617,578 electric smelting.pdf
09/15/2020 11:48 AM 36,392 electric-smelting-and-refining.pdf
09/15/2020 11:48 AM 944,494 EPA-ELECTROCHEMICAL GOLD EXTRACTION FROM THE RESIDUES OF VACUUM-THERMAL TREATMENT OF GOLDCONTAINING ANTIMONY ORES-2014.pdf
01/02/2020 09:06 PM 8,359,807 Extracting NPGM From Oxide Deposits.pdf
09/15/2020 11:48 AM 1,417,774 Extraction of Gold, Then, Now, Future.pdf
03/23/2016 11:26 PM 6,831,933 extraction-process-carbonaceous-gold-ore.pdf
05/17/2021 03:19 AM 9,884,906 Extractive_Metallurgy_of_Copper_G_W_DAVE.pdf
01/28/2020 11:58 AM 415,806 Final+-+Smelting+and+Refining.pdf
08/16/2023 07:10 AM 57,492,865 fire assay gold silver lead ores.pdf
03/23/2016 03:49 AM 30,726 FIRE ASSAY.pdf
02/04/2019 09:56 AM 5,129,853 Gold Casting Alloys.pdf
03/22/2016 09:11 PM 990,792 Gold Extraction and Recovery Processes.pdf
09/16/2011 12:21 AM 660,526 gold in watchmaking.pdf
03/29/2016 07:50 PM 58,159,905 Gold Mining and Milling in the United States and Canada - Current Practices and Costs.pdf
03/23/2016 10:15 PM 5,612,648 Gold process mineralogy.pdf
04/19/2020 08:39 AM 3,617,814 Gold Prospecting Equipment.mhtml
02/04/2012 06:29 AM 2,878,743 GOLD REFINING FORUM HANBOOK VOL 1.pdf
01/17/2021 03:36 PM 87,184 Gold Smelting Flux.pdf
01/31/2023 09:44 AM 1,777,230 GOLD TRANSPORT BY COMPLEX METAL CHLORIDE VAPORS.PDF
01/03/2020 07:59 AM 58,554 gold-leach-smelt-techniques.rtf
09/15/2011 06:44 PM 627,758 GOLD-liquid.pdf
01/24/2011 04:29 AM 1,062,819 GoldExtaction.pdf
10/10/2019 10:56 PM 990,792 Gold_Extraction_and_Recovery_Processes.pdf
09/15/2011 06:43 PM 149,069 Gold_Flash.pdf
01/07/2011 06:43 PM 2,670,734 Gold_Recovery_Butyl_Diglyme[1].pdf
02/04/2012 06:47 AM 4,915,200 GOLD_REFINING_FORUM_HANDBOOK_VOL_2.doc
12/30/2010 06:10 PM 426,308 GREEN CHEMISTRY APPROACH FOR LEACHING GOLD.pdf
12/25/2010 01:33 AM 109,741 Haber Gold Process leaching.pdf
12/27/2010 08:10 PM 47,759,190 Handbook_of_metallurgy.pdf
11/15/2014 09:17 AM 13,917,757 Handbook_of_Milling_Details.pdf
05/16/2020 10:00 PM 1,339,590 Heap_leaching_as_a_key_technology_for_recovery of values from low-grade ores.pdf
03/23/2016 02:38 AM 1,220,298 Hydrometallurgical recovery of valuable metals.pdf
03/23/2016 02:36 AM 4,442,147 HYDROMETALLURGY & SOLUTION MINING.pdf
03/27/2016 12:00 AM 6,453,600 hydrometallurgy of mercury sulfide ores.pdf
12/30/2010 03:28 AM 2,153,919 iGOLIBOOKLET (2).pdf
02/20/2020 01:31 PM 5,401,289 Implementation_of_sodium_hydroxide_pretr.pdf
08/26/2020 07:23 AM 2,605,614 2011-A Carbonaceous Sedimentary Source-Rock Model for Carlin-Type and Orogenic Gold Deposits.pdf
03/23/2016 01:38 AM 785,847 A mineralogical investigation of refractory gold ores and their beneficiation, with special reference to arsenical ores.pdf
10/08/2019 04:01 PM 616,537 Acidic_sulphate_leaching_of_chalcopyrite.pdf
03/23/2016 02:27 AM 286,284 ACIDIFIED FERRIC CHLORIDE LEACHING OF A CHALCOPYRITE CONCENTRATE.pdf
05/04/2016 05:16 AM 150,696 Ammoniacal thiosulphate leaching of gold ore.pdf
04/22/2020 02:21 PM 4,778,263 AN INVESTIGATION OF COPPER RECOVERY FROM A SULPHIDE OXIDE ORE WITH A MIXED COLLECTOR SYSTEM.pdf
05/23/2020 10:17 PM 15,725,723 AN INVESTIGATION OF LEACHING CHALCOPYRITE ORE.pdf
02/20/2020 01:31 PM 1,509,942 Application_of_Diagnostic_Leaching_Technique FOR REFRACTORY GOLD ORES.pdf
02/12/2019 10:57 AM 2,390,702 Arsenic Speciation Around Gold-Ore Roasters.pdf
10/23/2019 02:34 AM 527,826 A_Review_on_Novel_Techniques_for_Chalcopyrite Ore Processing.pdf
07/25/2020 02:17 AM 1,281,596 bioreduction_of_sulfide_minerals_to_recover_invis-wageningen_university_and_research_168827.pdf
03/23/2016 02:40 AM 1,159,653 chalcopyrite leached with ferric sulphate and SodiumChloride.pdf
12/28/2019 11:45 AM 350,029 Chalcopyrite_concentrate_leaching_with_biologically produced ferric sulphate.pdf
08/27/2020 02:37 PM 1,954,398 Characterization and kinetic study on ammonia leaching of complex copper ore.pdf
07/25/2020 02:17 AM 1,206,923 Characterization of an iron oxyhydroxide (gossan type) bearing refractory gold and silver ore by diagnostic leaching.pdf
05/09/2016 10:23 AM 981,446 Characterization of refractory behaviour of complex goldsilver ore by diagnostic leaching.pdf
10/09/2019 02:07 AM 1,419,577 Characterization_of_refractory_behaviour complex gold-silver ore by diagnostic leaching.pdf
03/23/2016 01:13 AM 2,188,075 CHEMICAL SPECIATION OF GOLD IN ARSENOPYRITE.pdf
10/09/2019 02:07 AM 432,535 Chemical_Transformations_of_Metals_Leaching from Gold Tailings.pdf
05/10/2016 06:57 PM 331,070 CHLORIDE-HYPOCHLORITE OXIDATION AND LEACHING OF REFRACTORY SULFIDE GOLD CONCENTRATE.pdf
03/23/2016 02:24 AM 468,391 Chlorination Solutions Of Chalcopyrite Concentrate.pdf
03/23/2016 11:08 PM 961,696 Desulpherization-of-mine-tailings.PDF
03/23/2016 01:29 AM 367,117 Dialnet-QuantificationOfRefractoryGoldInGrainsOfPyriteAndA-3944257.pdf
05/10/2016 06:47 PM 551,765 DISSOLUTION KINETICS OF PYRITE ORE BY HYDROCHLORIC ACID.pdf
03/23/2016 11:16 PM 318,336 Effect of pH on Pulp Potential and Sulphide Mineral Flotation.pdf
12/28/2010 08:28 AM 481,285 ENVIRONMENTAL GEOCHEMISTRY OF SKARN AND POLYMETALLIC CARBONATE.pdf
01/02/2020 09:07 PM 11,843,637 Examination of Micro-Scale Inter- and Intra-Sulphide Distribution and Its Relation to Geometallurgy.pdf
06/04/2020 12:51 AM 2,785,740 Extracting Gold from Auriferous Pyrites-1874.pdf
03/23/2016 11:12 PM 6,063,766 Flotation Chemistry of Complex Sulphide Ores.pdf
06/04/2020 12:51 AM 2,646,526 Fool's Gold- Pyrite Tells the Smart Things about Jinguashi Gold Mine.pdf
10/09/2019 02:07 AM 214,243 Fundamentals_and_applications of alkaline sulfide leaching and recovery of gold.pdf
10/09/2019 02:07 AM 533,858 Galvanic_Effect_of_Pyrite_on_Chalcopyrite Leaching in Sulfate-Chloride Media.pdf
08/26/2020 07:23 AM 2,143,819 Geochemistry and metallogeny of Neoproterozoic pyrite in oxic and anoxic sediments.pdf
07/26/2020 09:08 AM 14,759,616 Gold bearing Polymetallic Veins and Replacement Deposits.pdf
03/23/2016 01:13 AM 1,646,194 GOLD IN MASSIVE SULFIDES.pdf
06/04/2020 12:51 AM 835,676 GOLD IN MICHIGAN.pdf
02/20/2020 01:31 PM 4,479,871 Gold-bearing_arsenopyrite_and_pyrite_in refractory ores.pdf
03/23/2016 12:56 AM 469,740 Gold-in-pyrite-barker-Econ-Geol-2009.pdf
04/12/2020 08:21 AM 1,339,590 Heap_leaching_as_a_key_technology_for_recovery of values from low-grade ores.pdf
03/03/2016 05:26 PM 3,898,044 High-Sulfidation Epithermal Pyrite-Hosted Au (Ag-Cu) Ore Formation.pdf
06/04/2020 12:51 AM 475,151 hydrometallurgical-technology-for-gold-recovery-fromrefractory-goldbearing-raw-materials-and-the-solutionto-problems-of-subsequent-dehydration-processes-.pdf
03/27/2016 12:00 AM 6,453,600 hydrometallurgy of mercury sulfide ores.pdf
04/22/2020 02:21 PM 6,706,744 Improved Flotation of Bastnaesite and Chaclcopyrite.pdf
10/15/2019 06:33 PM 1,375,149 Improving of copper extraction from chalcopyrite by using NaCl.pdf
03/29/2016 07:37 PM 12,217,079 Innovations in Copper Leaching Employing Ferric Sulphate-Sulphuric Acid.pdf
03/26/2016 11:38 PM 2,964,890 INTRUSION-RELATED POLYMETALLIC CARBONATE DEPOSITS.pdf
10/08/2020 11:53 AM 5,204,527 Invisible and microscopic gold in pyrite Methods and new data for massive sulfide ores of the Urals_2015.pdf
03/03/2016 03:10 AM 11,492,999 Iron Oxide Copper-Gold Deposits.pdf
10/29/2019 12:27 AM 569,251 IRON_CONTROL_IN_HYDROMETALLURGY.pdf
12/14/2010 12:34 AM 7,020,760 j01_polymetallic_mantos_ag_pb_zn.pdf
01/02/2020 09:07 PM 575,510 LEACHING KINETICS OF COPPER FROM CHALCOPYITE CONCENTRATE IN NITROUS-SULFURIC ACID.pdf
03/30/2016 01:18 AM 8,718,015 Leaching Nonsulphide Copper Ores with Sulphur Dioxide.pdf
03/23/2016 03:11 AM 6,128,260 leaching-refractory-ore.pdf
10/09/2019 02:07 AM 413,378 Leaching_of_an_oxide_gold_ore_with_chloride - hypochlorite solutions.pdf
10/09/2019 02:07 AM 424,181 Leaching_of_chalcopyrite_with_ferric_ion General aspects.pdf
01/30/2019 09:08 PM 1,095,001 Metamorphism of Polymetallic Deposits.pdf
06/04/2020 12:51 AM 1,037,388 Mineral chemistry of polymetallic mineralization associated with altered granite.pdf
06/04/2020 12:51 AM 1,937,914 MINERAL PREPARATION OF SULPHIDE ORES FROM ALASKA.pdf
06/04/2020 12:51 AM 7,606,068 Mineralogy and Pretreatment of a Refractory Gold Deposit in Zambia.pdf
04/22/2020 02:21 PM 5,924,893 Mitigation of environmental hazards of sulfide mineral flotation.pdf
05/21/2016 10:26 PM 1,212,592 Options to Treat Refractory Ores.pdf
03/23/2016 04:32 AM 4,176,441 oxidation of ores.pdf
03/23/2016 11:24 PM 212,382 OXIDATIVE LEACHING OF SULFIDE ORES.pdf
03/23/2016 02:53 AM 20,532,283 Physicochemical Problems of Mineral Procssing.pdf
03/20/2016 01:48 PM 5,333,089 Polymetallic Vein and Replacement Deposis-part2.pdf
03/16/2016 11:33 PM 1,043,341 Polymetallic Vein and Replacement Deposis.pdf
10/29/2019 12:27 AM 492,176 Process_options_in_the_treatment_of_a_mied atacamite, secondary copper.pdf
05/10/2016 06:48 PM 1,456,373 Properties of pyrite and associated iron sulphides.pdf
03/23/2016 10:22 PM 5,409,250 Pyrite Content in Copper-Gold Ore Treatment.pdf
03/23/2016 11:19 PM 14,644,052 reactions-of-refractory-gold-ores.pdf
01/29/2019 02:04 PM 4,077,546 RECOVERING GOLD BY ROASTING.pdf
06/04/2020 12:51 AM 159,132 Recovering Gold from Copper Concentrate via the HydroCopperTM Process.pdf
02/25/2011 01:28 PM 267,883 Recovery of precious metal values from ores.pdf
02/25/2011 01:25 PM 247,940 Recovery of precious metals from difficult ores 2.pdf
02/25/2011 01:23 PM 347,072 Recovery of precious metals from difficult ores.pdf
02/25/2011 01:29 PM 534,262 Recovery of precious metals from metal sulphides.pdf
03/29/2016 11:02 PM 30,132,164 Recovery of Zinc from Low-Grade and Complex Ores.pdf
03/22/2016 09:04 PM 981,446 refractory behaviour of complex ore.pdf
08/02/2020 09:13 AM 14,717,953 Review of extraction, processing, properties applications of reactive metals.pdf
03/29/2016 06:01 PM 580,063 Review on Novel Techniques for Chalcopyrite Ore Processing.pdf
03/23/2016 02:32 AM 465,598 Roasting and chlorine leaching of gold-bearing refractory concentrate.pdf
05/05/2016 09:00 AM 5,422,207 Roasting-of-Gold-and-Silver-Ores-1870.pdf07/25/2020 02:17 AM 3,624,439 SGS MIN 2012 04 Recovering refractory reources EN 13 09.pdf
10/23/2019 02:34 AM 920,669 Silver_catalyzed_IBES_process_application copper-zinc sulphide concentrate.pdf
03/26/2016 11:37 PM 481,285 SKARN AND POLYMETALLIC DEPOSITS.pdf
03/17/2016 05:52 AM 126,280 SULFIDE HYDROMETALLURGICAL.pdf
08/07/2020 07:20 AM 20,100,358 Sulfide Mineralogy and Geochemistry (Reviews in Mineralogy and Geochemistry 61) by David J. Vaughan (z-lib.org).pdf
03/23/2016 01:59 AM 16,380,425 SULPHIDE MINERAL CHEMISTRY.pdf
10/03/2019 05:20 AM 5,675,527 Sulphide_mineral_flotation_a_new_insight.pdf
03/23/2016 11:25 PM 1,971,682 Sulphidic Mine Tailings.pdf
07/25/2020 02:17 AM 9,396,323 The influence of mineralogy and surface chemistry on flotation of Cortez complex carbonaceous double refractory gold ore.pdf
02/20/2020 01:31 PM 777,672 The_Application_of_Roasting_Pretreatment for Antimonial Refractoty Gold and Silver Ores.pdf
10/03/2019 05:20 AM 386,337 The_dissolution_of_chalcopyrite_in_chlor.pdf
02/20/2020 01:31 PM 1,009,827 The_effecT_of_Iron_And_oxIdIzIng_flux_Addition on The fIre AssAy of low grAde PyrITIc Refractory Gold Ores.pdf
11/15/2014 10:03 AM 11,506,158 The_enrichment_of_sulphide_ores.pdf
10/09/2019 02:07 AM 101,494 Thiosulfate_leaching_of_silver_gold_from_complex sulfide concentrates.pdf
03/16/2016 11:31 PM 243,582 TI IRON OXIDE CU-U-AU-REE DEPOSITS.pdf
03/23/2016 03:15 AM 1,396,802 Treatment and Microscopy of Gold and Base Metal Ores.pdf
10/27/2019 07:59 AM 2,786,556 Treatment_of_A_Copper-Rich_Gold_Ore_by_Canide_Leaching.pdf
06/06/2020 04:43 AM 780,938 US4416692-PROCESS FOR EXTRACTING GOLD, SILVER, PLATINUM, LEAD, OR MANGANESE METALS FROM ORE.pdf
08/12/2020 08:28 AM 693,691 US4892631-RECOVERY OF PRECIOUS METALS FROM COMPLEX ORES.pdf
09/15/2011 07:03 PM 547,449 What Are Refractory Metals.pdf
06/06/2020 04:43 AM 596,898 WO1995031577A1-Process for Extracting Gold and Silver from Auriferous Pyrites and Arsenopyrites.pdf
03/22/2016 09:34 PM 7,536,404 behaviour of free gold in flash flotation.pdf
04/22/2020 02:21 PM 10,694,240 COLLECTORLESS FLOTATION OF CHAlCOPYRITE AND SPHALERITE ORES.pdf
11/09/2020 03:49 PM 207,066 Current_Trends_in_Gravity_Separation_Tecnology_for_Fine_Gold_Recovery.pdf
 
Back