If using sulfuric cell,you must break the outer tube. Otherways you dont get the gold from inside.
Inner part is hard bronse alloy. It breaks easily with a light hit. Outer tube is softer. it will be flattened if you hit it. I will make test bath when i got some free time. I`ll let you know.