I have a muslin cloth as the anode filter
Graphite cathode 2" x 0.8"
About 80gl electrolyte previously used for about 300g of 98-99% pure silver
Tried the cell at 2.5v, 1.8v, 3.5v and the Amps were about, 0.33, 0.21, 0.58.