Newbie here. Please define SMD. Perhaps a photo. I have been looking over you guys shoulder for awhile. Thanks to everyone for sharing selflessly. Much respect.lazersteve said:For ceramic K6's I don't crush or break them up, I simply remove the aluminum heat spreader (if present) and the SMD's and process away. The SMD's easily come off with a chisel or a set of wide mouth cutters. Leverage the SMD's against the edge of the cpu die (chisel) or the edge of the cpu housing (wide pliers) and they will pop right off. Do this over a large plastic bag to collect the SMD's.
Steve
TY muchsnoman701 said:SMD = Surface Mount Device
Such as MLCC (multi layer ceramic capacitor)
As opposed to axial capacitor or CERDIP ceramic dual inline package IC (integrated circuit)
TY. I appreciate the responseanachronism said:It's actually far quicker to soak the AMD procs (without the aluminium lids, don't ever do them with the lids) in HCl and the SMDs will drop off.
How about the Pins. Do I need to remove them first? Or process on AR with them on?rickzeien said:TY. I appreciate the responseanachronism said:It's actually far quicker to soak the AMD procs (without the aluminium lids, don't ever do them with the lids) in HCl and the SMDs will drop off.
Sent from my LG-H872 using Tapatalk