S scrapparts Well-known member Joined Jun 23, 2016 Messages 142 Oct 24, 2016 #1 Can someone tell me how much Nitric Acid is needed to Dissolve 1lb of clean no#1 copper? Thanks scrapparts
Can someone tell me how much Nitric Acid is needed to Dissolve 1lb of clean no#1 copper? Thanks scrapparts
4metals Moderator Staff member Supporting Member Moderator Joined Apr 5, 2009 Messages 6,196 Location northeast USA Oct 24, 2016 #2 That should take 64 fluid ounces of Nitric (1/2 gallon)
S scrapparts Well-known member Joined Jun 23, 2016 Messages 142 Oct 24, 2016 #3 Thanks for the reply. scrapparts