kurt said:depends on the company - some companies only require a 500 lb minimum others as much as 3000 lbs --- processing fees will range from $.90 to $1.25 depending on company &/or lot size (meaning some companies have a flat per lb rate & others have a sliding scale where the processing fee goes down with more volume)
Also some companies have other charges (like assay fee &/or other fees) some companies don't
Most companies pay out on the Au - Ag - Pd & Cu but their pay out rates will differ --- I talked to only one company that also paid out on the tantalum (that was about 4 years ago & can't remember the company name - I "think" they were in Pa)
Kurt
solar_plasma said:In germany it's very common, that you can send them per kg. Although I guess that will not help. - It wonders me that it should be so different in the mightiest country of the world. :shock:
Not sure about the mightiest country in the world, but many things are different here. :|solar_plasma said:In germany it's very common, that you can send them per kg. Although I guess that will not help. - It wonders me that it should be so different in the mightiest country of the world. :shock:
Smack said:Gotta get the sample of your material people, you should be there for it or have a rep. there for you. That way if you don't like the numbers you can have your sample assayed and go from there.
Claudie said:I think it was CJ Environmental that I sent some boards to last year. I am pretty sure they are the Cash for Gold people and pay like the Cash for Gold company does. If I remember right, I averaged about 09 cents per pound on the material I sent. Thanks for the information on the others.
Smack said:Gotta get the sample of your material people, you should be there for it or have a rep. there for you. That way if you don't like the numbers you can have your sample assayed and go from there.