Hello ! Is there anyone who can tell me how to precipitate Palladium from Cyanide ? thanks !
Lino1406 said:Pd cyanide sometimes contain ammoniac. Hence needed hood. Al, Zn, Cu will do that
Lino1406 said:Order of magnitude: 10% weight
Lino1406 said:When an oxidizer (O2 or H2O2) is present the reaction is swift, no preference for any metal is observed although theoretically silver is preferable, next palladium, next gold
Lino1406 said:Obvious. Rhetorical question?
anachronism said:Lino1406 said:Pd cyanide sometimes contain ammoniac. Hence needed hood. Al, Zn, Cu will do that
How much Pd does it take up please Lino?
razvanflorin said:anachronism said:Lino1406 said:Pd cyanide sometimes contain ammoniac. Hence needed hood. Al, Zn, Cu will do that
How much Pd does it take up please Lino?
Thanks for answer but i'm looking for a kind of powder percipitant like.. we use Sodium Dithionit for gold.. i want something for palladium.