Dude4ever said:
Water obviously have a higher vapor pressure than plastics :lol:
At room temperature, sure. At the boiling point of water too, but at incineration temperature it's close to even. Water and plastic would have the same vapor pressure when your reactor breaks, it's just a question of a minor difference in temperature. The biggest difference is that water isn't flammable but pyrolyzed plastic vapors are.... or in words that a dude would understand. Big kaboom!

This is Not a joke!

Göran
 
Incineration and Pyrolysis is two very different things. Incineration is a thermochemical reaction by heat and oxygen to convert carbon to carbon dioxide. Pyrolysis is a thermochemical reaction to decompose organic material in the absence of oxygen leaving carbon behind.
 
The moderators would like to thank all of the members that contributed to the original thread upon which this thread was based, as well as those that asked questions showing what was missing. Because of the extra length and interest in this thread we have created the above consolidated version making for an easier read. We encourage all members to read, comment, and ask questions in the original thread, Incineration

The Library threads should not be considered to constitute a complete education. Instead, they're more like reading a single book on the subject of recovery and refining. There is so much more information on the forum, and it is impossible to include it all in these condensed threads. Members are strongly encouraged to read the rest of the forum to round out their education.
 
Status
Not open for further replies.

Latest posts

Back
Top