The residue left over from leaching the original mineral concentrate contains rhodium, iridium, ruthenium, and osmium. This is treated with molten sodium bisulfate to convert the rhodium to rhodium sulfate. The rhodium is then solubilized by water leaching, separated from the insolubles, and precipitated from solution by reduction with zinc powder. The crude rhodium metal product is converted to a soluble salt by treatment with chlorine and sodium chloride at high temperature, dissolved in water, precipitated with sodium nitrite, filtered, redissolved, and reprecipitated with ammonium chloride. This final precipitate is reduced to a pure metal powder.