Hello guys,
Here I will post pictures of the material and the construction of my electric kiln.
Here is the PID (controller) with the thermocouple, K type.
[IMG:1024:768]http://i18.tinypic.com/6nvlzzo.jpg[/img]
This is the front view of the controller.
The first row is the current temperature and the second is the desired temperature.
More pics will come later.
Thanks
Here I will post pictures of the material and the construction of my electric kiln.
Here is the PID (controller) with the thermocouple, K type.
[IMG:1024:768]http://i18.tinypic.com/6nvlzzo.jpg[/img]
This is the front view of the controller.
The first row is the current temperature and the second is the desired temperature.
More pics will come later.
Thanks