Shark Well-known member Joined Jun 8, 2014 Messages 2,999 Location Alabama May 11, 2017 #1 Although it isn't pretty, here it is.
S scrapman1077 Well-known member Joined Nov 4, 2007 Messages 248 Location north Alabama May 11, 2017 #2 Looks Great !
FrugalRefiner Administrator Staff member Administrator Supporting Member Moderator Joined Jan 14, 2012 Messages 6,480 Location Ohio, USA May 11, 2017 #3 How can you say it isn't pretty? That's gold shaming! :twisted: You should be ashamed of yourself. Send it to me. I'll give it the appreciation it deserves. Dave
How can you say it isn't pretty? That's gold shaming! :twisted: You should be ashamed of yourself. Send it to me. I'll give it the appreciation it deserves. Dave
T Topher_osAUrus Well-known member Joined Feb 16, 2016 Messages 1,923 Location OK DoC May 11, 2017 #4 I think shark is fishing.. For compliments that is. I think its gorgeous!
UncleBenBen Well-known member Supporting Member Joined Sep 2, 2015 Messages 733 Location Nashville, TN May 11, 2017 #5 It ain't pretty he says!! Shark, sell that puppy quick! Then find a good ophthalmologist....STAT!!! :shock: :lol: 8) :G Nice job man! :G
It ain't pretty he says!! Shark, sell that puppy quick! Then find a good ophthalmologist....STAT!!! :shock: :lol: 8) :G Nice job man! :G
Shark Well-known member Joined Jun 8, 2014 Messages 2,999 Location Alabama May 11, 2017 #6 No more doctors! I have a very bad appointment tomorrow, test results that couldn't be discussed over the phone. Never had that happen before. But thanks guys, this one was a lot easier to get done.
No more doctors! I have a very bad appointment tomorrow, test results that couldn't be discussed over the phone. Never had that happen before. But thanks guys, this one was a lot easier to get done.
anachronism Well-known member Joined May 31, 2016 Messages 3,166 May 12, 2017 #7 Well done and also good luck today.