Here she is, 26.9 grams. Over half the weight came from eyeglass frames and the rest from mixed gold filled jewelry.


IMG_0707.JPG
 
Sold it today and was happy with the results. I now use a small percentage to pick up some better equipment. I now have a vacuum pump and a 2 gallon reservoir tank to go with it. A few fittings and a gauge, it should be ready to go.

Here is a shot of the XRF reading just for the fun of it. It did read the same on both sides as well.

26.9 grams xrf.jpg
 