J jons007 Member Joined Aug 3, 2022 Messages 24 Location Suisun City Aug 4, 2022 #1 Does anybody know how to process Niobium, titanium and copper wire mix?
L Lou Moderator Staff member Moderator Joined Nov 4, 2007 Messages 5,217 Location Rhodia Drive Aug 4, 2022 #2 Into what? TiNbCu reminds me of NMR windings.
J jons007 Member Joined Aug 3, 2022 Messages 24 Location Suisun City Aug 5, 2022 #3 Hi, into niobium, someone told me it needs to be heated up to burn out the copper and titanium.But thI dont know the dangers of refractory metals..
Hi, into niobium, someone told me it needs to be heated up to burn out the copper and titanium.But thI dont know the dangers of refractory metals..
L Lou Moderator Staff member Moderator Joined Nov 4, 2007 Messages 5,217 Location Rhodia Drive Aug 5, 2022 #4 Well niobium and titanium burn to oxide starting before the copper melts.
J jons007 Member Joined Aug 3, 2022 Messages 24 Location Suisun City Aug 6, 2022 #5 so how do i do it.Or do you know someone who can do it for me..