samuel-a
Well-known member
- Joined
- Oct 7, 2009
- Messages
- 2,190
All,
I have what i suspect is Pd powder which contains significant amounts of H.
The powder is dry and includes a small carbon contamination (a rough estimate would be 0.5-3% W:W).
Heating the powder causes violant eruptions which shoots powder and sparkes all over the place.
I'm trying to treat the material and bring it to simple Pd powder but avoiding chemically leaching the Pd or thermaly "decompose" it.
Any ideas?
I have what i suspect is Pd powder which contains significant amounts of H.
The powder is dry and includes a small carbon contamination (a rough estimate would be 0.5-3% W:W).
Heating the powder causes violant eruptions which shoots powder and sparkes all over the place.
I'm trying to treat the material and bring it to simple Pd powder but avoiding chemically leaching the Pd or thermaly "decompose" it.
Any ideas?