Hi all. Had some conflicting results and am curious as to the numbers and returns people are getting on average form ram and cpu's. From poor Ram, only gold fingers, rest all copper and misc. returned 2.5g ish on 100 sticks. My reaction where heavily faulted though, using sodium nitrate to react with sulfuric to distill nitric. Was then expecting perhaps 8- 10g per 200 with the Ram that has all gold throughout the exposed metals. I was only able to recover about a gram. I was trying that Subzero shor stuff... Its just sodium nitrate and no substitute for nitric... The subzero though dose not recommend a pre-nitric bath though like typical recovery. Trying to precipitate gold with such a heavily contaminated solution was a nightmare. I just ended up dropping 3 can of aluminum in and precipitating everything for a better recovery process in the future. A lye, then nitric batch, then regia to fix this one
But anyway per 100 sticks 3 - 5g a typical recovery rate you guys finding? or how about for CPU's?
Curious too from 100g filled you would expect 20g of 24k new. I'm sure not 1/20th is recovered. How much typical wear is being found? 10- 15 g return? Thanks I'll continue to post as I get more results..
But anyway per 100 sticks 3 - 5g a typical recovery rate you guys finding? or how about for CPU's?
Curious too from 100g filled you would expect 20g of 24k new. I'm sure not 1/20th is recovered. How much typical wear is being found? 10- 15 g return? Thanks I'll continue to post as I get more results..