Got my parcel in the mail from California today. Just unpacking and taking pictures and notes for each of the incoming materials.
Looks beautiful! All of it!
Microwave parts -1144 grams
Cylindrical pins - 717g
Pronged pins - 1503g
Partial plate pins - 1092g
Gold traces - 1083g
'sim cards' -776g + 69g
Gold mylar pieces -124g
Ceramic processors -654g
The "sim cards" arent really sim cards, I cant recall exactly what they came from, arcade machine cards I think?
Anyways, I will keep updating this thread with pictures as I go, I believe to start. The traces and pronged pins will be first in nitric. While the other pins will be getting treated for traces of solder.
I, of course, have more pics, but I need to trim them down and get them a much more reasonable size before putting them on here.
Thread will be updated after I get some of it going, and then have the chance to post up.
Thank you all again, without each of you here, I would never have learned this valuable trade, and would have never gotten this wonderful opportunity.
Looks beautiful! All of it!
Microwave parts -1144 grams
Cylindrical pins - 717g
Pronged pins - 1503g
Partial plate pins - 1092g
Gold traces - 1083g
'sim cards' -776g + 69g
Gold mylar pieces -124g
Ceramic processors -654g
The "sim cards" arent really sim cards, I cant recall exactly what they came from, arcade machine cards I think?
Anyways, I will keep updating this thread with pictures as I go, I believe to start. The traces and pronged pins will be first in nitric. While the other pins will be getting treated for traces of solder.
I, of course, have more pics, but I need to trim them down and get them a much more reasonable size before putting them on here.
Thread will be updated after I get some of it going, and then have the chance to post up.
Thank you all again, without each of you here, I would never have learned this valuable trade, and would have never gotten this wonderful opportunity.