48 hours 47 minutes in action
Entire beaker slightly greenish tint
Anode basket 3/4 full
Good silver growth on the edges
Seems like Silver particles in solution
Had to shut it last night
Slimes dropped on the crystals twice
Looks like the plastic coating on the wire started to deteriorate .
Cleaning up , cementing 1/2 the electrolyte out
Cement silver looks great
Probably the last time using the graphite anode
Cement silver from half the electrolyte
Left pictures is from cement silver less then 24 hours much cleaner
Right was left in for a week , more copper in the silver cement
Lessons learned
Time for stainless steel bowl
new crucible (ordered )
Found lead and tin in one sample
99.43/ 97/94
Didn’t keep track of the ugly bars when melting into bigger bar drag