hi everybody !
i am newbie at metal refining and the first steps that i made i have some questions
i decide to use this method
a.dissolve Ag to HNO3
b.add NaCl to produce AgCl
c.carefully wash AgCl with water
d.put Na2Co3 at AgCl, heat the mix at oven 400-420 C
e.wash again the mix and take out the NaCl
f.final dry, and then melting
The questions are :
1.Before i put the Na2Co3 i must dry the AgCl or is it ok if it is wet?
2.Does anyone follow this procedure , and have some remarks to make?
yours opinions will be very helpfull to me
thank you
i am newbie at metal refining and the first steps that i made i have some questions
i decide to use this method
a.dissolve Ag to HNO3
b.add NaCl to produce AgCl
c.carefully wash AgCl with water
d.put Na2Co3 at AgCl, heat the mix at oven 400-420 C
e.wash again the mix and take out the NaCl
f.final dry, and then melting
The questions are :
1.Before i put the Na2Co3 i must dry the AgCl or is it ok if it is wet?
2.Does anyone follow this procedure , and have some remarks to make?
yours opinions will be very helpfull to me
thank you