I decided to share these photos of the best yielding material known personally to me in category: pins

снп34 USSR connectors - looking barely mid-grade, shooting more than 30g/kg Au :)
Local old TESLA black WK stand back with "just" 10g/kg Au.

That said, one female connector yielding more than 0,4g Au :D I am still wondering why they did this. This isn´t any special series of this connector, any MIL spec. nothing "unusual"... Regular connectors. Some types more than 40g/kg... But, I am happy :)
 

Attachments

  • IMG_20220912_221509.jpg
    IMG_20220912_221509.jpg
    4.3 MB · Views: 0
  • IMG_20220912_221709.jpg
    IMG_20220912_221709.jpg
    3.8 MB · Views: 0
Connectors have been my favorite material to date. Those look to be some damn fine pins.
You do not find this scrap very often, as old USSR appliances here weren´t that prevalent since we had a domestic factories here. Which produced also fine connectors (some aiming higher than 14g/kg, average around 8), but nowhere 30g/kg :D

Personally, I much more like old ceramic ICs - very little metal and very good gold content. Effective, low acid consumption... Cleaner work :) but with 3% gold pins, I can´t complaint
 