kadriver
Well-known member
I decanted my stock pot and made a short video of it
https://youtu.be/cm2nd_NB0GI
It looks like quite a bit of black mud!
kadriver
https://youtu.be/cm2nd_NB0GI
It looks like quite a bit of black mud!
kadriver
g_axelsson said:I have only refined my stock pot once, I went straight to AR and precipitated the gold, the remaining liquid had some PGM:s in it so I cemented it out with zinc and saved the black powder for later refining.
Here is a reminder of an old post...
http://goldrefiningforum.com/phpBB3/viewtopic.php?f=52&t=21273&p=219523#p219526
Göran
nickvc said:The only advantage is to separate the Pd from the Pt which as I pointed out depends on the amount likely to be in the stock pot, if there is only a few grams of both metals then yes straight to AR, I think if you used cold weak AR you might well still leave the Pt behind undissolved so long as he keeps the reaction cold.
Enter your email address to join: