jimdoc said:Is this the oven you cook your food in? Like in your kitchen?
The one I used had been in storage for the last three years. Since we moved, that oven no longer fit anywhere reasonable at our new place. I dug it out for this purpose, but found that there were no stains, no smells, and no corrosion.
Is baking PCBs in aqueous sodium hydroxide in an oven used for cooking really a bad idea?
On YouTube, there was this dude with a... magnificent beard... who did just that. Granted, his whole demeanor made me want to do more research, but I figured that lye was just a cleaning agent... and inside the oven... shouldn’t be too bad, right?