Can somebody tell me what the exact composition is of BGA from ram? I can't find it in it's exact form on the forum. I ask this question because I want to know what oxides there will be formed after incineration.
I see to many times that people don't take proper precautions, they create clouds of dust in their gardens or they drain waste water away.
As far as I know the dust of these BGA chips consists of the following (in various oxide states):
ironoxide
copperoxide
tinoxide
zinkoxide
leadoxide
(cadmiumoxide??)
Maybe also some metals in their pure state.
Some sillica compunds
Some carbon compounds will be left, depending on the succes of the incineration step.
What do you guys do with the water after bleu bowling? Just sette out the oxides and decant the water??
I see to many times that people don't take proper precautions, they create clouds of dust in their gardens or they drain waste water away.
As far as I know the dust of these BGA chips consists of the following (in various oxide states):
ironoxide
copperoxide
tinoxide
zinkoxide
leadoxide
(cadmiumoxide??)
Maybe also some metals in their pure state.
Some sillica compunds
Some carbon compounds will be left, depending on the succes of the incineration step.
What do you guys do with the water after bleu bowling? Just sette out the oxides and decant the water??