Ragnor said:So If I had a sodium sulfate solution and a copper cathode and used the nugget as an anode. Would that theoretically pull the copper into solution and onto the cathode and leaving my values as a sludge? does that cut it for a possible method?
Ragnor said:My thinking on the sodium sulfate is that I have it handy and it will create an acidic solution. When voltage is applied I should get a copper sulfate solution formed in the container.
This seams to be a method discussed on the internet for copper refining.
.
I thought sodium is more reactive than copper, which means the sodium would stay in solution while the copper stays put?Ragnor said:My thinking on the sodium sulfate is that I have it handy and it will create an acidic solution. When voltage is applied I should get a copper sulfate solution formed in the container. This seams to be a method discussed on the internet for copper refining.
Is there any potential for evolving any deadly or highly toxic gasses with this method? I am seeing a white mist puff off of the top of the container as bubbles burst on top of the solution.
Ragnor said:So, the using the NASO4 adding sodium sulfate to water yields sulfuric acid, correct? sulfuric acid and copper makes copper sulfate. Now the part I don't know about is the effect of the Na on the solution. My assumption was that it would just act as a charge carrier. If I am mistaken please correct me.
.
Eftersom vissa personer försöker att uppfinna ett bättre hjul... utan att först ha lärt sig hur ett hjul fungerar.Cerber said:К чему такие сложности?
Не проще ли растворить самородок и восстановить палладий в виде аминохлорида палладия? Медь при этом останется в растворе.
Enter your email address to join: