PureMarble
Member
Hello I joined this forum to get to know a little bit or maybe a lot of this business, I invested with a friend who owns several mines. We have a gravity separation facility which works mainly with precious metals like gold and PGMs being Iridium one of the most present of them all.
We have tested 1 ton concentrate from 50 milled tons and have had up to 2.6kg of Iridium itself apart from lots of other metals. This were done on 150 mesh but were told 400 mesh will give us 4x more product. This tests have been done in well respected Mexican universities and private labs.
There is not much tech or knowledge of this type of metals in Mexico so I would like to know what do you think I should do next or who should I contact. I was looking at Sibanye, Anglo American, Umicore?
TIA
We have tested 1 ton concentrate from 50 milled tons and have had up to 2.6kg of Iridium itself apart from lots of other metals. This were done on 150 mesh but were told 400 mesh will give us 4x more product. This tests have been done in well respected Mexican universities and private labs.
There is not much tech or knowledge of this type of metals in Mexico so I would like to know what do you think I should do next or who should I contact. I was looking at Sibanye, Anglo American, Umicore?
TIA