Hi Folks,I would appreciate any help you could give me. My Silver Crystal has a brown tint. The middle photo shows a sample compared with a sample from a previous batch.
The Cell has been running at 2.5v which at its max was giving 2.2 amp with new 150g/l Electrolyte.
I am presuming that because of this discolouration I will need to run it through the Cell again, If so can I put it in the Basket as it is or do I need to make it into Bars?
Many thanks.
The Cell has been running at 2.5v which at its max was giving 2.2 amp with new 150g/l Electrolyte.
I am presuming that because of this discolouration I will need to run it through the Cell again, If so can I put it in the Basket as it is or do I need to make it into Bars?
Many thanks.