hi!

this is my latest product,this was finished a week ago, i've done this with the help of my loving wife.. :oops:

scrap: rejected chip resistors.

process: scrap dissolved by diluted nitric acid, Ag chloride converted with iron in battery acid, refined with cuppelation process.

weight: 3208 grams.

again, credits goes to Steve, Harold and GSP.

thank you very much guys!

meng
 

Attachments

  • 19012011047.jpg
    19012011047.jpg
    169.4 KB
  • 19012011048.jpg
    19012011048.jpg
    124.7 KB
Wow!

You've been busy.

Are you going to run it through the Silver Cell next to get the purity?

Steve
 
hi Steve!

no, i won't run it in a silver cell, you will notice the pipe? thats the indications of buyers acceptable purity.

nothing is very complicated for them in buying metals from me. :wink:

i have already my own Agcell, maybe some other time i would use it for my master pieces. :lol:

thanks to you again Steve!

meng
 
Any idea of the gross weight of the resistors you started with?

I must have millions of these little critters myself of all diferent sizes. I have been wondering if there was anything of value in them.

Texan
 
Did you try to test for Pd during process? That look so cool that I am putting some in acid as we speak and tomorrow will test them with DMG. :)
 
hi!

i have here half ton of tiny chip, tinier the better, i actually do the 100 kilos per batch for a day.

it was a funny story about these chips. once,i have a sample of this chip, i researched about this, google gave the pdf file for the technical documentation of the item, i found silver!

so i tried to roast it in a cupola type dish and i started to cupel it.

as i drive the lead, i figured that it has a silver in it!

large batch followed. :twisted:

i recover it with dilute nitric.

no further testing for Pd.

meng.
 
PM me your address if you want, or address of some of your friend. I will send you 20ml of DMG Testing solution courtesy of goldrefiningforum and of course me :)... :lol: That will last you for at least hundred tests.
You can test your acids and wastes just to be sure that you do not discarding something 40x more valuable.
 
It depend on how you test. Few ml in test tube, dilute with water so tested solution is not brown or black but fairly clear and few drops of DMG. Then it will not be hard to spot yellow (Pd).
 
jaun said:
Be careful, DMG also precipitates nickel, usually red, but in dirty solutions its difficult to tell.

DMG precipitates Nickel in a Basic solution and Palladium in an Acid solution. One just has to keep an eye on the pH.
 
Can you post a picture of those rejected chip receptors so i can see what they look like? i don't know what they are and seem to be a source of silver so im curious thanks.

-Adam
 
jaun said:
Be careful, DMG also precipitates nickel, usually red, but in dirty solutions its difficult to tell.


As long as your solution is acidic you won't get any pink (nickel) when testing with DMG.

Steve
 
That's the biggest piece of refined silver I've ever seen, here on this forum or anywhere else. Great job. If you don't mind, send me one of those :shock:

I'm going to have to save that photo. That's just too big to handle.

Kevin
 

Latest posts

Back
Top